# Lambar Filin Ita Ce Ƙayyadaddun: Tsire-tsire 55, 19.92% EL Cracks

> Wani bincike na tsire-tsire 55 ya auna fashewar EL a cikin 19.92% na modules da wurare masu zafi a cikin 1.51%. Bambancin tsakanin tsire-tsire, sau 350, shine adadin da ya cancanci yin aiki akai.

![Lambar Filin Ita Ce Ƙayyadaddun: Tsire-tsire 55, 19.92% EL Cracks](https://cdn.ooitech.com/static/upload/image/20261026/field-el-crack-hot-spot-rates-55-plant-survey.png)

- ** Ƙungiyar Edita ta Ooitech
- ** 2026-11-17
- ** 0 Ra'ayoyi
- ** [Ajiyar Makamashi & Aikace-aikace](./Energy-Storage.html)

Alhakin edita na wannan labarin yana hannun **Wuhan Ooi Photoelectric Technology Co., Ltd.** An rubuta kuma an duba shi daga ƙungiyar edita ta Ooitech. Duba [manufar edita](/editorial-policy.html) don yadda muke rubutu, inda ake amfani da kayan aikin AI, da yadda za a nemi gyara.

## Lambar Filin Ita Ce Ƙayyadaddun: Tsire-tsire 55, 19.92% EL Cracks

**Amsa mai sauri:** Wani binciken taron 2026 ya yi samfurin tsire-tsire 55 na kasar Sin a yankuna shida kuma ya auna hanyoyin gazawa biyu daban: electroluminescence akan tsire-tsire 29, infrared na drone akan 33. Fashewar da EL ke iya gani sun kai matsakaicin 19.92% na modules kowace shuka, wurare masu zafi sun kai matsakaicin 1.51%. Fiye da rabin tsire-tsire sun kasance sama da 10% fashewa kuma hudu cikin goma sun kasance sama da 1% wurare masu zafi. Matsakaicin shine mafi karancin amfani a cikinsa. Mafi kyawun shuka ya auna 0.15% fashewa, mafi muni 52.63%, bambancin kusan sau 350, kuma wurare masu zafi sun bazu fiye da sau 2,000. Tsire-tsire da ke jigilar modules masu kama da juna suna zama nesa da juna da tsari biyu na girma, wanda ke nuna kulawa, sanyawa da aikin aunawa maimakon fasahar tantanin halitta. Abin da ke biyo baya shine abin da binciken ya auna, abin da takaitaccen bayani ba zai iya gaya muku ba, da yadda za a juya adadin zuwa kasafin kurakurai kowane matakin samarwa.

Kowane module yana barin masana'anta da hoton electroluminescence da tambarin wucewa. Shekaru goma bayan haka drone ya sami fashewa a cikin module daya cikin biyar. Nisan da ke tsakanin wadannan gaskiyoyi biyu shine abin da wannan binciken ke aunawa.

## Abin da binciken ya auna a zahiri

Ƙungiyar ta zaɓi tsire-tsire 55 da kai ba tare da wani zaɓi ba a yankunan arewa maso yamma, arewa maso gabas, arewa, gabas, kudu da tsakiya, wanda ya shafi shekaru daban-daban na haɗawa da wutar lantarki da nau'ikan tsire-tsire daban-daban. An gudanar da bincike biyu daban-daban a lokaci guda, wanda shine abu na farko da za a lura da shi: ba a auna tsage-tsage da wuraren zafi a kan tsire-tsire ɗaya ba.

- **EL a kan tsire-tsire 29:** hoton electroluminescence na modules, wanda aka duba don tsage-tsage a cikin sel.
- **Drone infrared a kan tsire-tsire 33:** binciken zafi na iska, wanda aka duba don modules da suka fi maƙwabtansu zafi.

Ma'aunin kwatancen sun haɗa da shekarun haɗawa da wutar lantarki, yanayin ƙasa, yanayin amfani kamar agrivoltaics, da yanki. Ba a ware fasahar sel ba. Takardar taƙaitaccen taro ce, don haka lambobin da ke ƙasa su ne waɗanda taƙaitaccen ya bayyana, ba cikakken bayanan ba.

## Matsakaicin biyu, da kuma dalilin da ya sa su ne abin da ba daidai ba

Tsagewa ya kai kashi 19.92% na modules a kowace masana'anta a matsakaici. Wurare masu zafi sun kai kashi 1.51% a matsakaici. Idan aka karanta su a matsayin kanun labarai, lambar farko tana nuna cewa module ɗaya cikin biyar yana da tsagewar da ake gani, na biyun kuma yana nuna cewa wurare masu zafi ba su da yawa. Dukansu karatun biyu daidai ne a fasaha amma ba su da amfani a aikace, domin babu ɗayansu da ke bayyana rarrabuwar.

Rarrabuwar ita ce binciken. Tsagewa ya kasance daga kashi 0.15% a masana'anta mafi tsafta zuwa kashi 52.63% a mafi muni. Wurare masu zafi sun kasance daga kashi 0.003% zuwa kashi 8.89%. Masana'antu biyu na iya bayar da rahoton cin jarrabawar masana'anta kuma su sami bambanci na tsari uku na girma a binciken fili. Matsakaici a cikin wannan yawan ba ya bayyana kowace masana'anta ta musamman.

Ƙididdigar ma'aunin tana faɗin abu ɗaya da ƙarfi. Kashi 58.62% na masana'antun EL da aka auna sun fi kashi 10% tsagewa, wato 17 cikin 29. Kashi 40.54% na masana'antun infrared da aka auna sun fi kashi 1% wurare masu zafi. Lambar da rabin yawan ya zarce ita ce bayanin yawan, ba gargaɗi game da keɓewa ba.

| Alama | Tsagewar EL | Wurare masu zafi na infrared na jirgi mara matuƙi |
| --- | --- | --- |
| Masana'antun da aka bincika | 29 | 33 |
| Matsakaicin kaso na modules | 19.92% | 1.51% |
| Iyaka | 0.15% zuwa 52.63% | 0.003% zuwa 8.89% |
| Masana'antun da suka zarce ma'auni | 58.62% sun zarce 10% | 40.54% sama da 1% |
| Matsakaicin mafi kyau zuwa mafi muni | kusan sau 350 | fiye da sau 2,000 |

## Abubuwa huɗu da binciken ya ambata

Binciken ya danganta ƙimar biyu da masu canji huɗu, kuma tsarin ya yi daidai da yadda waɗannan lahani suke samuwa.

Gargaɗi ɗaya kafin jerin. Waɗannan alaƙa ne da aka auna a kan samfurin 55, ba kwatancen da aka sarrafa ba. Ita ma masana'anta ɗaya na iya zama tsohuwa, mai tsaunuka da ƙura a lokaci guda, kuma bincike irin wannan ba zai iya danganta wani kaso na 19.92% ga wani abu guda ba. Abin da zai iya yi shi ne ya gaya maka inda za ka fara duba idan naka adadin ya zo da yawa.

### Shekaru

Dukansu ƙimar suna ƙaruwa da shekarun haɗin grid. Wannan ya dace da rayuwar tsagewa: ƙaramin tsagewa yana farawa a busbar ko gefen tantanin halitta, yana faɗaɗa ƙarƙashin zagayowar zafi da inji, sannan yankin tantanin da ya keɓe ya daina ba da gudummawa. Tsagewar da ba ta keɓe wani abu ba tana fitowa iri ɗaya a hoton EL, wanda shi ya sa shekaru ke ƙara adadin da ake gani da sauri fiye da yadda suke motsa wutar lantarki.

### Ƙasa

Tsire-tsire na tsaunuka sun fi auna mafi girma don tsagewa, wanda takardar ta danganta ga ƙasa da canjin zafin jiki. Sufuri da sarrafawa sau biyu abu ne mai yiwuwa ƙari: wurin tsauni yana nufin hanya mai tsawo, ƙarin canja wuri da tushen rak da zai iya karkatar da firam wanda ya kasance lebur lokacin da ya bar masana'anta.

### Yanayin

Tsire-tsire na agrivoltaic sun fi auna mafi girma don wurare masu zafi. Inuwar amfani, ƙarin zafi a ƙarƙashin tsarin da tara ƙura duk suna turawa a hanya ɗaya, kuma inuwa ita ce abin da ke juya tsagewar da ke akwai zuwa tushen zafi na gida. Ilimin lissafi na yadda tantanin da aka yi inuwa ke shiga cikin juzu'i na baya kuma ya yi zafi ya cancanci karantawa daban daga ƙididdiga; duba [me yasa inuwa da wurare masu zafi ba abu ɗaya ba ne](https://www.ooitech.com/does-shading-always-cause-solar-hot-spots-reverse-bias.html).

### Yanki

Arewa maso yamma sun fi auna mafi girma a duka biyu. Babban canjin yini, haske mai yawa, yashi da iska ke ɗauka da ajiyar ƙura sune bayanin da aka saba, kuma suna aiki akan tsagewa da wurare masu zafi ta hanyoyi daban-daban: canji yana motsa faɗaɗa tsagewa, ƙazanta yana motsa inuwar da ke sa tantanin da ya tsage ya yi zafi.

Hanyoyin biyu ba a rarraba su daidai a cikin ƙirar tantanin ba. Tsarin tantanin da ke yada wutar lantarki ta juyi a kan babban yanki yana yin sanyi a daidai rabon inuwa, wanda hakan ɗaya ne daga cikin dalilan da ba za a iya kwatanta adadin wuraren zafi a tsakanin tashoshi ba tare da kwatanta abin da aka girka ba. Kwatancen [jurewar inuwa a cikin ƙirar tantanin](https://www.ooitech.com/why-do-bc-solar-cells-offer-better-shading-tolerance-and-lower-hot-spot-temperature.html) ya shafi wannan tsarin.

## Abubuwa huɗu da taƙaitaccen bayanin ba zai iya gaya maka ba

Takardar tana da gaskiya game da iyakokinta, kuma waɗannan iyakoki sun cancanci a ɗauka cikin kowane shawara.

- **Tsanani ba ya cikin adadin.** Tsagewar da ake gani tana daga ɗan siririn layi wanda ba ya keɓe wani yanki har zuwa yankin tantanin da ya katse gaba ɗaya. Masana'antar tana auna waɗannan A, B da C don wani dalili. Tasha mai kashi 20% wadda galibi aji A ce ba ɗaya ce da tasha mai kashi 8% wadda aji C ce.
- **Ba a raba fasahar tantanin ba.** Taƙaitaccen bayanin bai raba PERC, TOPCon da HJT ba, haka kuma kaurin wafer, adadin busbar, ko gilashi-backsheet da gilashi-gilashi. Waɗannan su ne ainihin abubuwan da mai yin module zai so na gaba.
- **Kashi ɗaya ba ya rabawa.** 58.62% daidai yake 17 cikin 29, wanda ya dace da samfurin EL. 40.54% ba ya rabuwa cikin tsire-tsire 33: 13 cikin 33 shine 39.4% kuma 14 cikin 33 shine 42.4%. Yana rabuwa cikin 15 cikin 37. Mai yiwuwa ma'aunin wurin zafi ba 33 bane, kuma har sai cikakken takardar ya tabbatar da hakan, ɗauki kaso na ƙofar wurin zafi a matsayin kimanin.
- **Shekaru suna ɗauke da tsara.** Tsofaffin tsire-tsire kuma suna amfani da tsofaffin modules da aka gina bisa tsofaffin ƙa'idoji kuma aka girka bisa tsofaffin al'ada. Tasirin lokaci da tasirin tsara sun haɗu, kuma babu wani binciken fili na wannan siffa da zai iya raba su.

## Me yasa ingantaccen sakamakon EL na masana'anta ba ya hasashen wannan

Hoton EL na masana'anta ma'auni ɗaya ne a lokaci ɗaya, wanda aka ɗauka kafin a tattara module ɗin, a jigilar shi, a ɗaga shi, a matse shi da a loda shi. Duk abin da ke faruwa bayan haka ba a iya gani a gare shi, kuma yawancin fashe-fashen da ke cikin fili ana ƙirƙirar su ne a can.

Wannan ba hujja ba ce cewa hoton masana'anta ba shi da amfani. Hujja ce cewa hoton yana tabbatar da wani abu mafi ƙunci fiye da yadda masu siye suke tsammani: yana tabbatar da cewa module ɗin ya bar layin ba tare da wani aibi da layin zai iya ganowa ba, a matakin da layin yake amfani da shi. Adadin fili yana taruwa ne daga ƙofar zuwa gaba, don haka kwatanta shi da adadin wucewa na masana'anta kwatanta adadi biyu ne daban-daban.

Hankali ya cancanci jumla ta kansa, domin shi ne inda tsire-tsire biyu da suke da nau'ikan module iri ɗaya suke samar da kaso daban-daban. Hoton hasken lantarki da aka ɗauka a ƙaramin ƙarfin turawa na gaba, tare da kyamara mara inganci ko ɗan gajeren lokacin fallasa, ba zai iya gano ƙaramin tsagewar da wannan module ɗin yake nunawa a ƙarƙashin ɗaukar hoto a hankali ba. Babu wani abu da ya canza game da module ɗin. Karatun ne ya canza.

Muna gudanar da binciken hasken lantarkinmu a ci gaba da ƙarfin turawa na gaba tare da saitunan fallasa na dogon lokaci don gano ƙananan tsage-tsage da wuri, don tabbatar da an rubuta ƙananan lahani kafin modules su bar wurin masana'anta.

Wannan kuma shine dalilin da ya sa ya kamata a karanta 0.15% da 52.63% na binciken a matsayin bayani game da tsire-tsire, ba kawai game da modules ba. Wurin da yake karanta hotunansa cikin sauƙi zai bayar da rahoton ƙimar da take da kyau sosai kuma zai sami labarin bambancin a jirgin drone na shekaru goma. Kayan aiki da tsari don hoto na kan layi da na waje an rufe su a [bayaninmu kan kayan gwajin EL da IV](https://www.ooitech.com/solar-panel-el-tester-and-vi-tester-machine-opt-m960b-m951b-m950b-ooitech-solar-module-el-testing-equipment.html), da kuma faffadan jerin gwaje-gwaje a [jerin gwajin aminci](https://www.ooitech.com/pv-module-reliability-tests-list-cell-vs-module-failure-causes.html).

![ƙimar tsage-tsage da wurare masu zafi a fili](https://cdn.ooitech.com/static/upload/image/20261026/field-el-crack-hot-spot-rates-55-plant-survey.png)

## Inda tsage-tsage suke shiga bayan ƙofar

Kusan kowane inji da ke ƙasa sananne ne, kuma kowanne yana da wurin da za a iya auna shi. Dalilin jera su shi ne cewa lambar filin ita ce jimillar matakai biyar, kuma shukar da ke auna huɗu daga cikinsu za ta iya danganta na biyar.

Stringer da layup suna saita yawan farko ta hanyar damuwa na soldering da dimples na ribbon, wanda ya dogara da yadda ake yin ribbon ɗin da kuma tin ɗinsa kamar yadda ya dogara da tashar soldering. Lamination yana ƙara damuwa a gefe kuma, a lokacin da ba daidai ba, yana haifar da ramuka tare da ribbon. Packing da transport suna ƙara nauyin kusurwa da tari waɗanda na'urar rikodin girgiza za ta rubuta. Installation yana ƙara ƙarfin clamp, karkatar mount da kuma wani lokacin ƙafa. Service yana ƙara nauyin dusar ƙanƙara, girgizar iska da kuma zagayowar zafi waɗanda ke tsawaita duk abin da ke can. [Don hana lamination daga ba da gudummawa ga adadin lahani na 19.92%, muna tsara zagayowar matsa lamba mai matakai da yawa da kuma daidaitaccen hawan zafin jiki don guje wa damuwa a gefen tantanin halitta da kuma kawar da ramuka tare da ribbon.](https://www.ooitech.com/how-pv-ribbon-is-made-drawing-annealing-and-tinning.html) as much as of the soldering station. Lamination adds edge stress and, at the wrong ramp, voids along the ribbon. Packing and transport add corner and stacking loads that a shock logger would record. Installation adds clamp torque, mount twist and the occasional foot. Service adds snow load, wind vibration and the thermal cycles that extend whatever is already there.

To prevent lamination from contributing to the 19.92% defect rate, we program multi-stage pressure cycles and uniform temperature ramps to avoid cell edge stress and eliminate voids along the ribbon.

Sufuri shine matakin da aka fi barin shi a cikin kasafin kuɗi kuma mafi arha wajen kayan aiki. Na'urar rikodin girgiza da karkata a cikin kwandon jigilar kaya tana kashe ƙasa da sake karanta EL ɗaya na modules ɗin da take karewa, kuma tana mai da shakku mara tushe zuwa kwanan wata, hanya da kololuwar hanzari. Wuraren da suke karɓar modules ta hanyar doguwar hanyar tsaunuka su ne ainihin waɗanda binciken ya samu a saman teburin tsagewa.

## Kasafin kuɗin lahani da za ka iya rubutawa

Fitowar aiki ta bincike irin wannan ba kaso da aka yi niyya ba ce. Rabe ne. Ba wa kowane mataki kaso, ma'auni da mai shi, sannan lambar filin ta zama abin da masana'anta za su iya yin muhawara a kansa maimakon abin da kawai za su iya bayar da rahoto a kansa.

| Mataki | Babban inji | Abin da za a auna | Mai shi |
| --- | --- | --- | --- |
| Stringer da layup | Damuwar solder a busbar, dimple na ribbon | EL na cikin layi bayan stringer, kowane shift | Ingancin layi |
| Lamination | Damuwar gefe, voids tare da ribbon | EL bayan lamination da gani | Injiniyan tsari |
| Marufi da sufuri | Tasirin kusurwa, nauyin jibgewa | Logger mai girgiza kowane jigilar kaya, samfurin EL na isowa | Dabaru |
| Shigarwa | Matsi fiye da kima, karkatar da abin ɗaure, tafiyar ƙafa | Binciken ƙarfin juyawa, samfurin EL bayan shigarwa | EPC |
| Sabis | Dusar ƙanƙara, girgizar iska, zagayowar zafi | Binciken infrared na shekara da binciken IV na igiya | O da M |

## Abin da za a auna, da yadda za a kimanta shi

Dokoki biyu suna sa lambobin filin su zama masu kwatantawa. Na farko shi ne a ba da rahoton rarraba matakin, ba adadin waɗanda suka ci ba. Hoton EL da aka karanta a matsayin ci ko faɗuwa yana watsar da bayanai guda ɗaya da ke da alaƙa da asarar wuta, wato ko tsagewar ta keɓe wani yanki.

Na biyu shi ne a ba da rahoton adadin gabaɗaya tare da kowane kashi. Wannan binciken yana nuna dalilin: 58.62% yana rabuwa cikin sauƙi zuwa 17 cikin 29, kuma 40.54% ba ya rabuwa zuwa 33 kwata-kwata. Rahoton filin da ya bayyana kashi ba tare da adadin ba ba za a iya bincika shi ba, kuma lambar da ba za a iya bincika ta ba a ƙarshe za a yi jayayya a kanta maimakon a yi aiki da ita.

Ga infrared, kwatancen ya dogara da yanayi. Bambancin zafin da ake gani yana motsawa tare da hasken rana, saurin iska da zafin muhalli, don haka binciken da aka yi a watan Yuli da wanda aka yi a watan Janairu ba ma'auni ɗaya ba ne. Kwatanta abin da ya dace da abin da ya dace, kuma ka ɗaure jadawalin da rashin aikin yi a matakin igiya maimakon da kalanda.

Doka ta uku tana da arha fiye da kowane ɗayan: ajiye hotunan. Ƙididdigar tsagewa ba tare da hoton da ke bayanta ba ba za a iya sake tantance ta ba idan abokin ciniki ya ƙalubalanci karatun, kuma kuɗin ajiya ba komai ba ne idan aka kwatanta da kuɗin sake tashi da shuka.

## Inda waɗannan lambobin suka fito

Kowane adadi a cikin wannan labarin ya fito ne daga takardar taro da ke taƙaita binciken bazuwar na tsire-tsire 55 na China, kamar yadda aka ruwaito a matakin taƙaitaccen bayani: tsire-tsire 29 don electroluminescence, 33 don infrared na jirgi mara matuƙi, a cikin yankuna shida da kewayon shekarun haɗin grid. Binciken bai bayyana fasahar tantanin halitta ko lissafin kayan aikin module ba, abin da muka lura da shi maimakon cika shi.

Lissafin lissafi da kasafin kuɗi na matakin mataki namu ne, an gina su daga hanyoyin aiki maimakon daga bayanan binciken. Bayanin game da 40.54% da ba ya rabuwa cikin tsire-tsire 33 bincike ne kan taƙaitaccen bayanin, ba da'awar cewa aikin da ke ƙasa ba daidai ba ne; yana nufin ƙila samfurin wurin zafi ya fi girma fiye da yadda taƙaitaccen bayanin ya faɗa.

Ka'idar rarrabawa, sharuɗɗan kwatance don infrared, da rabuwar mataki aiki ne na yau da kullum a binciken fili. Ba mu haɗa tazarar amincewa ga kowane adadi ba, saboda abstract ba ya ɗauke da ita.

## Tambayoyi da Amsoshi

### Tambaya: Menene 19.92% yake nufi, modules ko cells?

Modules. Ita ce matsakaici, a cikin tsire-tsire 29 da EL ta bincika, na rabon modules kowace shuka inda aka ga tsagewa a hoton. Ba adadin matakin cell ba ne kuma ba adadin asarar wuta ba ne.

### Tambaya: Shin tsagewar da ake gani koyaushe tana rage wuta?

A'a. Tana rage wuta ne lokacin da tsagewar ta keɓe wani yanki na cell daga hanyar wutar lantarki. Ƙaramin layi da ya ratsa busbar ba tare da yanke wani abu ba na iya zama a cikin module shekaru da yawa, kuma rarrabawa bisa tsanani ita ce hanyar da masana'antu ke raba waɗannan lokuta biyu.

### Tambaya: Me ya sa bambancin tsakanin tsire-tsire yake da girma haka?

Binciken yana nuni ga shekaru, ƙasa, yanayin wuri da yanki, kuma waɗannan gaskiya ne. Bambancin ninki 350 kuma yana buƙatar kulawa da aikin aunawa don bayyana shi: hanyoyin sufuri, horon hawa da ma'aunin hankali da ake amfani da shi wajen karanta hoton duk suna motsa adadin.

### Tambaya: Wace fasahar cell ce ta fi yawan tsagewa?

Takardar ba ta faɗi haka ba. Ba ta bayar da rabe-rabe ta PERC, TOPCon ko HJT ba, kuma ba ta bayar da rabe-rabe ta kaurin wafer, adadin busbar ko tsarin gilashi ba. Ƙananan wafer da manyan sifofi gabaɗaya sun fi sauƙin lalacewa, amma wannan binciken ba ya ƙididdige hakan.

### Tambaya: Shin za a iya hasashen wurare masu zafi daga bayanan tsagewa?

Kamar sharadi kawai. Tsagewa na haifar da hanyar wutar da za ta iya yin zafi a wuri ɗaya, kuma inuwa ce ke tura wutar ta cikinta. Binciken ya auna su biyun a samfuran shuka daban-daban, don haka ba zai iya bayar da adadin juyawa daga tsagewa zuwa wurare masu zafi ba.

### Tambaya: Samfuran nawa ne binciken waje ya kamata ya ɗauka?

Takardar ba ta fayyace tsarin samfuri ba. Abin da ta nuna shi ne cewa dole adadin jimillar ya kasance tare da sakamakon: 58.62% ya rabu zuwa 17 cikin 29, kuma 40.54% ba ya rabuwa zuwa 33. A wallafa adadin.

### Tambaya: Shin sakamakon infrared na jirgi mara matuƙi ana iya kwatanta shi tsakanin yanayi?

Ba kai tsaye ba. Bambancin zafin da ake gani ya dogara da hasken rana, iska da zafin muhalli, don haka kwatanta yanayi na haɗa lahani da yanayin sama. Tashi a yanayi iri ɗaya kuma a bi waɗannan igiyoyi ɗaya a kan lokaci.

### Tambaya: Me mai yin module ya kamata ya yi da wannan adadin?

Raba shi a cikin matakai biyar da za su iya haifar ko tsawaita tsagewa, ba kowane mataki ma'auni da mai shi, kuma bayar da rahoton EL ta maki maimakon ta ci ko fadi. Kashi ɗaya na manufa yana jawo jayayya; kasafin kuɗi yana jawo kayan auna.

## Tunani na ƙarshe

Lambar da ta fi amfani a wannan binciken ba 19.92% ba ce. Ita ce 350, rabon da ke tsakanin masana'anta mafi tsafta da mafi ƙazanta a cikin samfurin bazuwar 55. Modules masu kama da juna ba sa samar da wannan bambancin da kansu. Kulawa, hawa da kuma horon aunawa ne ke yin hakan, kuma waɗannan abubuwa ne da masana'anta za ta iya aunawa, tsara kasafin kuɗi da kuma bincika. Fara da bayar da rahoton adadin da ke bayan kowane kashi.

OOITech tana kera ɗaki ɗaya da biyu [injin laminator na panel na hasken rana](https://www.ooitech.com/solar-panel-laminator-machine.html) tare da tsarin zafi mai dumama da mai da wutar lantarki. Muna taimaka wa masu yin modules su rage damuwa na inji da ramuka ta hanyar daidaitaccen tsarin zafi da vacuum. Aika tarin module ɗinka, zanen kayan aiki, ko samfuran kayan zuwa ƙungiyar injiniyanmu don kimanta tsari da gwajin girke-girke.

---

##### Tags :

![](/template/ooitech/assets/img/shape/06.png)

![](https://cdn.ooitech.com/runtime/image/w800_h700_fitblur_v2_w800_h700_fitblur_v2_1757399770541443.webp)

### Nemi Farashi

Duk abubuwan da aka ɗora suna da tsaro kuma sirri ne.

## Muna isar da gwanintar da za ka iya amincewa sabis ɗinmu

Kayan aiki kai tsaye daga masana'anta.

![](/template/ooitech/assets/img/icon/money-2.svg)

### Fa'idodin Rage Kuɗi

Muna ba da ƙima ta musamman, muna haɓaka sakamako yayin da muke rage kasafin kuɗi ga abokan ciniki.

![](/template/ooitech/assets/img/icon/staff.svg)

### Ƙungiyar Ƙwarewarmu

Kwararrun ma'aikatanmu sun ƙware a sababbin hanyoyin magance matsaloli da dabarun da aka keɓance.

![](/template/ooitech/assets/img/icon/certified.svg)

### Fiye da Shekaru 15 na Ƙwarewar Masana'antu

Ƙwarewa mai zurfi tana tabbatar da sakamako masu dogaro, masu bin zamani, da tabbatattu don nasara.

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477357667605.webp )

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477724911512.webp)

![](/template/ooitech/assets/img/shape/06.png)

## Abin da Abokin Cinikinmu Ya ce game da mu

Shaidun abokan ciniki sun yaba da zurfin fahimtarmu game da ƙalubalen su, wanda ke haifar da sababbin hanyoyin magance matsaloli da riba mai ƙarfi. Haɗin gwiwa na dogon lokaci—wasu fiye da shekaru goma—suna nuna amincewarsu da gamsuwa. Labaran nasarar su suna motsa mu don ci gaba da wuce tsammanin su. [Ƙara Sani **](#quote-form)

![](/template/ooitech/assets/img/icon/quote.svg)

Godiya ga Ooitech don samar da kayan aikin gwajin ƙwayar hasken rana na BC da suka dace sosai.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1776426122864564.webp)

### KTECH

![](/template/ooitech/assets/img/icon/quote.svg)

Mutum mai babban rai. Na gode sosai da ziyarar ku Mista Wu. Na gode sosai da ayyukan da aka bayar wajen shigar da kayan aiki da horar da dalibai na. Mutum mafi kirki kuma ƙwararre a fanninsa.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041716444445.webp)

### Jizzakh Polytechnic Institute

![](/template/ooitech/assets/img/icon/quote.svg)

na gode da goyon bayan ƙwararrun ooitech da sabis na bayan lokaci.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1784509010217979.webp)

### Diarra Daga Afirka

![](/template/ooitech/assets/img/icon/quote.svg)

Na sake godewa sosai don babban taimako na inganta da gyara masana'anta da kuma koya wa ma'aikata yadda ake amfani da injinan

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1757479675272137.webp)

### Mark

BIPV Philippines

![](/template/ooitech/assets/img/icon/quote.svg)

Godiya ga Ooitech don samar da kayan aikin samarwa na atomatik cikakke—shigar da ku da sabis na bayan siyarwa sun yi kyau sosai.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041720921238.webp)

### Amjad

## Sabbin Kayayyakin Mu

![Layin Samar da Faifan Rana: Tsari daga 5 MW zuwa 1 GW](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032510951634.webp)

- [** ooitech](./solar-panel-production-line.html)
- [** 109](./solar-panel-production-line.html)

### Layin Samar da Faifan Rana: Tsari daga 5 MW zuwa 1 GW

Jagorar layin samar da faifan rana: tashoshi, rabin-atomati da atomati, tsarin 5 MW zuwa 1 GW, shimfidawa, kayan aiki, ma'aikata da shawarwarin RFQ.

![CHT9951A Mai Gwajin Hipot: Rufe Rukunin PV 0.1-10kV](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774601338282260.webp)

- [** Rachael](./cht9951a-cht9951b-solar-panel-hipot-insulation-resistance-tester-pv-module-safety-testing-equipment.html)
- [** 58925](./cht9951a-cht9951b-solar-panel-hipot-insulation-resistance-tester-pv-module-safety-testing-equipment.html)

### CHT9951A Mai Gwajin Hipot: Rufe Rukunin PV 0.1-10kV

CHT9951A/CHT9951B na'urar gwajin hipot da juriya ta insulation don gwajin PV module na hasken rana. Fitarwar DC har zuwa 10kV, juriya ta insulation har zuwa 99GΩ

![Layin Samar da Ribbon PV: Zana, Mirginewa, Tinning](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026051194879300.webp)

- [** ooitech](./pv-busbar-ribbon-integrated-drawing-rolling-tinning-production-line.html)
- [** 812](./pv-busbar-ribbon-integrated-drawing-rolling-tinning-production-line.html)

### Layin Samar da Ribbon PV: Zana, Mirginewa, Tinning

Ƙwararren layin samar da ribbon na PV busbar mai haɗawa wanda ya haɗa da zana waya, birgima, zana lebur, annealing da tsarin shafa tin don babban

![SS-2500B Tabber da Stringer: 2400 Cells/h, 3-20BB](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774258018905303.webp)

- [** ooitech](./SS-2500B-Full-Automatic-Solar-Cell-Tabber-Stringer-Machine-High-Speed-Production-Line-Equipment.html)
- [** 37139](./SS-2500B-Full-Automatic-Solar-Cell-Tabber-Stringer-Machine-High-Speed-Production-Line-Equipment.html)

### SS-2500B Tabber da Stringer: 2400 Cells/h, 3-20BB

SS-2500B cikakken atomatik tabber stringer inji don crystalline silicon solar cells tare da 2400PCS/H iya aiki, yana da infrared soldering

![Injin Ribbon PV: Zaren Waya don Ribbon Solar](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026051187922761.webp)

- [** ooitech](./wire-drawing-machine-for-solar-ribbon-production-line.html)
- [** 780](./wire-drawing-machine-for-solar-ribbon-production-line.html)

### Injin Ribbon PV: Zaren Waya don Ribbon Solar

Ƙwararren injin zana waya na tsakiya don layin samar da ribbon na hasken rana, yana da ƙirar kwance mai axis huɗu

![Cikakken Kayan Aikin Samar da Hasken Rana ta Atomatik](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774401482439949.webp)

- [** Rachael](./full-automatic-solar-panel-production-line-equipment-ooitech.html)
- [** 98980](./full-automatic-solar-panel-production-line-equipment-ooitech.html)

### Cikakken Kayan Aikin Samar da Hasken Rana ta Atomatik

Cikakken layin samar da hasken rana na Ooitech ya ƙunshi loda gilashi, shimfiɗa EVA, shimfiɗar igiya, manna tef, lamination, gyara, firam