# Ramukan Pinhole a cikin Ƙwayoyin TOPCon: Hanyar Mamaki

> Sabon bincike ya bayyana nau'ikan ramukan SiOx guda biyu a cikin ƙwayoyin TOPCon. Rufe ramukan da iskar oxygen da ta rage yana ƙara inganci zuwa 26.55%

![Ramukan Pinhole a cikin Ƙwayoyin TOPCon: Hanyar Mamaki](https://cdn.ooitech.com/static/upload/image/20260717/8f4e05ab43e74a832b2faee10f80bb99.webp)

- ** 2026-07-17
- ** 222 Dubawa
- ** [Blog](./Blog.html)

## Ramukan Pinhole a cikin Ƙwayoyin TOPCon: Hanyar Mamaki

**Amsa mai sauri:** Bincike kan ƙwayoyin TOPCon ya gano cewa barin wani adadi mai sarrafawa na siririn oxide da gangan na iya inganta passivation maimakon lalata shi, wanda hakan ya sauya wani zato da aka daɗe ana amfani da shi. Binciken ya auna yaduddukan oxide a cikin kewayon 0.2 nm da 0.3 nm idan aka kwatanta da ma'auni na 1.7 nm, kuma ya gano cewa siririn oxide ɗin da aka riƙe da gangan bai ƙara juriya kawai ba. Tunnel oxide a cikin ƙwayar TOPCon dole ne ya kasance siriri sosai don masu ɗauka su iya shiga ta cikinsa kuma ya kasance mai kauri sosai don passivate saman, kuma ma'aunin al'ada yana kan nanomita ɗaya ko biyu. Abin da sakamakon ya nuna shi ne cewa iyakar ba ta da kaifi kamar yadda aka zata, kuma yanayin sinadarai na mahaɗar yana da mahimmanci kamar kaurin. Ga layin samarwa, hakan yana juya hankali zuwa ga sarrafa mahaɗa maimakon kauri kawai.

PV Module Manufacturing · na Jerry, Ooitech

## Bayani

Ga wani abu da ke juya wani dogon zato a cikin silicon PV. Masu bincike sun gano cewa da gangan barin wasu "ramukan fil" a cikin SiOx Layer na wani [TOPCon](https://www.ooitech.com/what-is-topcon-solar-cell-a-complete-guide-to-tunnel-oxide-passivated-contact-technology.html) cell na iya tura inganci har zuwa 26.55%, maimakon jawo shi ƙasa.

Babban binciken: ƙananan ramuka a cikin oxide na tunnel sun rabu zuwa iyalai biyu. Ɗayan shine nau'in sake haɗawa (oxygen-depleted, inda poly-Si ke tuntuɓar c-Si kai tsaye, mara kyau), ɗayan kuma shine nau'in passivating (oxygen da ya rage yana zama a baya, yana passivating dangling bonds yayin da yake ba da damar tunneling, mai kyau). Nau'in passivating yana auna kusan 1.6 ± 0.2 nm × 1.4 ± 0.3 nm a cikin giciye, tare da yawan areal na 2 × 10¹² cm⁻². Wani samfurin Fischer ya nuna cewa abin da ke yanke shawarar aikin na'urar ba girman ramin ba ne, amma ko an yi passivation na ramin.

Tushen: *Passivating pinholes don manyan yanki da ingantattun hasken rana na silicon tare da tunnel oxide passivated contact*, Nat Commun 17, 2490 (2026). [https://doi.org/10.1038/s41467-026-70511-2](https://doi.org/10.1038/s41467-026-70511-2)

## Bayanan Bincike da Matsalar da Ta Tsaya

TOPCon yanzu shine babban tsarin n-type silicon. Runergy ya kai 26.55% akan 335 cm², Jinko ya tara TOPCon tare da perovskite zuwa 33.24%, kuma n-TOPCon mai gefe ɗaya yana da iyakar ka'idar 27.79%. Amma babu wanda ya tabbatar da rawar da ƙananan ramuka a cikin wannan SiOx Layer ke takawa.

Ra'ayin gargajiya: ƙaramin rami yana nufin poly-Si ya shiga cikin c-Si kai tsaye, passivation na oxygen ya gaza, labari mara kyau.

Gaskiyar ta fi rikitarwa. Oxide yayi kauri sosai (>1.7 nm) yana karewa da kyau amma ba ya iya wucewa da kyau, don haka FF ya rushe. Oxide yayi siriri sosai (<1.3 nm) yana nufin ƙarin pinholes, kuma yanzu kana damuwa game da rushewar Voc.

Marubutan sun raba kauri na oxide da rarraba iskar oxygen zuwa lokuta uku (sashen Gabatarwa):

- Hali na 1: oxide mai kauri, kariya yayi kyau, tunneling bai dace ba
- Hali na 2: oxide mai siriri tare da raguwar iskar oxygen, yana haifar da pinholes irin na sake haɗuwa (pinhole mara kyau na gargajiya)
- Hali na 3: oxide mai siriri amma iskar oxygen har yanzu tana shiga cikin pinhole, yana haifar da pinholes masu kariya (sabon binciken nan)

Kafin wannan, ƙudurin HR-TEM bai isa ya ga abubuwa ƙasa da 2 nm ba. Littattafai sun ba da rahoton diamita na pinhole daga 5 nm zuwa 200 nm da yawa daga 10⁶ zuwa 10⁸ cm⁻², waɗanda duk "manyan ramuka" ne. Selective etching da c-AFM sun dogara da bambancin saurin etching tsakanin Si da SiOx, don haka yankunan da ke da ragowar iskar oxygen ba sa buɗewa ta hanyar etching. Pinholes masu kariya an kawar da su ta hanyar waɗannan hanyoyin. Shi ya sa Hali na 3 ya daɗe ba a gani ba.

## Hanyar: Nau'ikan Pinhole Biyu (Hoto 2)

Aberration-corrected HAADF-STEM (JEM ARM200F plus Spectra 300, 200/300 kV) ya duba poly-Si/SiOx/c-Si interface a kan wafer mai inganci (25.40%) da kuma low-efficiency control (24.07%).

| Nau'i | Yanayin oxygen | Girma (high/low efficiency) | EELS O-K edge |
| --- | --- | --- | --- |
| Recombination | Oxygen-depleted, poly/c-Si lattice directly joined | Low-efficiency wafer ~1.37 × 1.35 nm | Deep oxygen valley |
| Passivating | Residual oxygen present, dangling bonds passivated | High-efficiency wafer 1.55 × 1.25 nm | Oxygen signal still visible, shallow oxygen valley |

### Mahimmin batu: pinholes a kan high-efficiency wafer a zahiri suna karami, kuma suna riƙe oxygen da kyau. Duk girman sun fi girma da oda guda goma fiye da yadda littattafan farko suka ruwaito.

Sakamakon samfurin Fischer point-contact (Fig. 3d a cikin asali):

- Yanki rami mai rami f = πr²/P², amma J₀ ba ya damuwa da f. Abin da ya fi rinjaye shi ne saurin sake haɗuwa da saman S a ramin.
- Kusan f ≈ 0.1, da zarar S ≳ 10³ cm/s, J₀ ya tashi da ƙarfi, kuma yana cika sama da S > 10⁵ cm/s.
- Ma'ana: mabuɗin babban aiki ba shine "sifili ramuka" ba, shine "ramuka da aka kare". Wannan shine babban haske na takarda gaba ɗaya.

A kan yawa, wannan ɗan juyin juya hali ne. Ƙididdiga daga X-Y orthogonal slicing a kan wafers 40 (high plus low efficiency) ya ba da 2 × 10¹² cm⁻² don karewa da 3 × 10¹² cm⁻² don ramukan sake haɗuwa, 4 zuwa 6 oda girma fiye da ƙimar adabi.

Dalilai uku sun taru: na farko, ra'ayi ya canza, don haka abubuwan da aka riga aka tantance sun zama bayyane; na biyu, samfuran wafers ne na masana'antu sama da 25%, ba tsarin gwaji ba; na uku, hanyar ita ce HAADF matakin atomic, kuma hanyoyin kai tsaye ba za su iya ganin yankin da ke ɗauke da oxygen sub-2 nm ba. Don kare kariya daga haɗuwa tare da jagorar haske daga samfuran TEM 50 zuwa 150 nm kauri, marubutan sun dawo da 4D-STEM ptychography tare da jagorar kauri, suna tabbatar da ƙididdigar yawa ba ta lalace ta hanyar tsinkayar tsinkaya ba.

## Wurin Sauya Tsari: Oxidation Mataki Biyu tare da Goge Bayan da Poly Triple Coupling

Abubuwan da aka samo daga Hanyoyin Asali da SI (Tebur na Ƙari 1):

- Oxidation mataki biyu: da farko O₂ oxidation zuwa bakin SiO₂, sannan matakin rashin isashshen oxygen (ba a shigar da oxygen ba). Nau'in mai wucewa yana buƙatar lokaci mai tsawo na kwararar oxygen, zafi mai girma, kwarara mai girma, da matsi mai girma, wanda ke taimakawa ga oxide mai daidaito da kauri.
- POCl₃ diffusion: rage zafin ajiya da ɗan gajeren lokaci yana inganta poly crystallization kuma yana hana sake haɗuwa na pinholes.
- Siffar goge bayan tana kan gaba da daidaiton kaurin oxide. Duk ukun dole ne a daidaita su tare don samar da Case 3 a tsaye.

## Kwatanta Ayyuka (Bayanan Hard Fig. 4)

Samfuran poly-Si/SiOx mai gefe biyu mai daidaitacce (n-Si 1–3 Ω·cm, goge gefe biyu):

- τeff: 8.9 ms babban inganci vs 2.96 ms sarrafawa (injection 5×10¹⁵ cm⁻³)
- J₀: 2.6 vs 10.6 fA/cm²
- ΔVoc da aka auna a 15.9 mV, amma bambancin J₀ kadai yana bayyana kusan ~11 mV. Sauran ~5 mV marubuta sun danganta ga ingantaccen rayuwar SRH na bulk. Tsarin annealing da aka inganta, yayin da yake haifar da pinholes masu rufe fuska, kuma yana cire ƙarfe masu gurɓata (suna ambaton aikin Krügener na 25% POLO). Gyara duka interface da bulk tare shine girke-girke don wuce 25%.

Ga FF, bambancin ya fi fitowa daga Rs:

- Rs: 357 (high efficiency) vs 619 mΩ·cm² (control), Suns-Voc measured
- ρc (TLM): 4.6 vs 5.4 mΩ·cm²

Maganar da ba ta dace ba: ta hanyar tunanin "pinholes masu yawa suna rage ρc", ƙarin pinholes masu rufe fuska a kan wafer mai inganci ya kamata ya rage ρc, kuma hakika 4.6 < 5.4. Amma marubuta sun ƙara wani juyi. Kusa da pinholes masu sake haɗuwa, phosphorus yana yaduwa cikin wafer, yayin da nau'ikan rufe fuska ke toshewa da oxygen (tsarin doping EDS a cikin Supplementary Fig. 10). Don haka tsarin doping da juriyar lamba suna bin dabaru daban-daban guda biyu, kuma ba za ku iya bayyana su da yawan pinhole kadai ba.

PL ya kasance daidai a duk faɗin wafer, kuma taswirar Corescan na rarraba Voc shima ya riƙe don daidaiton babban yanki.

## Layi ɗaya don Masana'antu

Wannan takarda tana tura hanyar sadarwa ta TOPCon daga labari na binary na "oxide mara lahani vs zubar da pinhole" zuwa na uku: "pinholes na iya zama masu kyau kuma, muddin oxygen yana nan". Abin da masana'antar ke buƙatar yi na gaba ba shine damuwa game da rashin pinholes ba, amma daidaita sarkar polishing na baya zuwa oxidation zuwa poly deposition domin pinholes su ɗauki oxygen. Wafer na Daheng a 25.40% akan 333.3 cm² ya riga ya tabbatar da hanyar tana aiki.

## Ra'ayin Ooitech

Abin da ya ba mu mamaki a nan shi ne yadda wannan ya dogara da sarkar tsari, ba kawai ƙirar tantanin ba. Wannan oxidation mai matakai biyu, daidaita POCl₃, da polishing na baya duk suna buƙatar tafiya tare shine irin haɗin da ke ɓacewa lokacin da aka haɗa layi guntu-guntu. A gefen module muna ganin irin wannan tsari, inda haƙurin lamination da stringing ke yanke shawarar ko tantanin mai kyau zai riƙe Voc ɗinsa. Idan kuna son kallon kusa kan yadda waɗannan matakai masu mahimmanci na hanyar sadarwa ke fassara zuwa filin samarwa na gaske, ziyarar mu na masana'anta akan YouTube ([www.youtube.com/ooitech](http://www.youtube.com/ooitech)) sun cancanci biyan kuɗi.

---

##### Tags :

![](/template/ooitech/assets/img/shape/06.png)

![](https://cdn.ooitech.com/runtime/image/w800_h700_fitblur_v2_w800_h700_fitblur_v2_1757399770541443.webp)

### Nemi Farashi

Duk abubuwan da aka ɗora suna da tsaro kuma sirri ne.

## Muna isar da gwanintar da za ka iya amincewa sabis ɗinmu

Kayan aiki kai tsaye daga masana'anta.

![](/template/ooitech/assets/img/icon/money-2.svg)

### Fa'idodin Rage Kuɗi

Muna ba da ƙima ta musamman, muna haɓaka sakamako yayin da muke rage kasafin kuɗi ga abokan ciniki.

![](/template/ooitech/assets/img/icon/staff.svg)

### Ƙungiyar Ƙwarewarmu

Kwararrun ma'aikatanmu sun ƙware a sababbin hanyoyin magance matsaloli da dabarun da aka keɓance.

![](/template/ooitech/assets/img/icon/certified.svg)

### Fiye da Shekaru 15 na Ƙwarewar Masana'antu

Ƙwarewa mai zurfi tana tabbatar da sakamako masu dogaro, masu bin zamani, da tabbatattu don nasara.

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477357667605.webp )

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477724911512.webp)

![](/template/ooitech/assets/img/shape/06.png)

## Abin da Abokin Cinikinmu Ya ce game da mu

Shaidun abokan ciniki sun yaba da zurfin fahimtarmu game da ƙalubalen su, wanda ke haifar da sababbin hanyoyin magance matsaloli da riba mai ƙarfi. Haɗin gwiwa na dogon lokaci—wasu fiye da shekaru goma—suna nuna amincewarsu da gamsuwa. Labaran nasarar su suna motsa mu don ci gaba da wuce tsammanin su. [Ƙara Sani **](#quote-form)

![](/template/ooitech/assets/img/icon/quote.svg)

Godiya ga Ooitech don samar da kayan aikin samarwa na atomatik cikakke—shigar da ku da sabis na bayan siyarwa sun yi kyau sosai.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041720921238.webp)

### Amjad

![](/template/ooitech/assets/img/icon/quote.svg)

na gode da goyon bayan ƙwararrun ooitech da sabis na bayan lokaci.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1784509010217979.webp)

### Diarra Daga Afirka

![](/template/ooitech/assets/img/icon/quote.svg)

Mutum mai babban rai. Na gode sosai da ziyarar ku Mista Wu. Na gode sosai da ayyukan da aka bayar wajen shigar da kayan aiki da horar da dalibai na. Mutum mafi kirki kuma ƙwararre a fanninsa.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041716444445.webp)

### Jizzakh Polytechnic Institute

![](/template/ooitech/assets/img/icon/quote.svg)

Godiya ga Ooitech don samar da kayan aikin gwajin ƙwayar hasken rana na BC da suka dace sosai.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1776426122864564.webp)

### KTECH

![](/template/ooitech/assets/img/icon/quote.svg)

Na sake godewa sosai don babban taimako na inganta da gyara masana'anta da kuma koya wa ma'aikata yadda ake amfani da injinan

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1757479675272137.webp)

### Mark

BIPV Philippines

## Sabbin Kayayyakin Mu

![Na'urar Laminator BIPV Mai Dakuna Biyu Mai Layer Daya](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774438506273987.webp)

- [** Rachael](./single-layer-double-chamber-automatic-bipv-laminator-otcy-2754dd-ooitech-solar-panel-lamination-equipment.html)
- [** 63298](./single-layer-double-chamber-automatic-bipv-laminator-otcy-2754dd-ooitech-solar-panel-lamination-equipment.html)

### Na'urar Laminator BIPV Mai Dakuna Biyu Mai Layer Daya

Ooitech OTCY-2754DD Single Layer Double Chamber Automatic BIPV Laminator yana da wuraren lamination guda biyu na 2700x5400mm, dumama biyu na sama da ƙasa

![SS-2500B Mai Haɗa Igiyar Tabbatacce: 2400 Kwayoyin rana/h, 3-20BB](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774258018905303.webp)

- [** ooitech](./SS-2500B-Full-Automatic-Solar-Cell-Tabber-Stringer-Machine-High-Speed-Production-Line-Equipment.html)
- [** 36928](./SS-2500B-Full-Automatic-Solar-Cell-Tabber-Stringer-Machine-High-Speed-Production-Line-Equipment.html)

### SS-2500B Mai Haɗa Igiyar Tabbatacce: 2400 Kwayoyin rana/h, 3-20BB

SS-2500B cikakken atomatik tabber stringer inji don crystalline silicon solar cells tare da 2400PCS/H iya aiki, yana da infrared soldering

![OSLB-1300 BC Cell Stringer: Kwayoyi 1000/sa'a, ±0.10mm](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032311945973.png)

- [** ooitech](./oslb-1300-back-contact-cell-welding-machine-bc-solar-cell-stringer-for-ibc-abc-hpbc-panel-production.html)
- [** 98960](./oslb-1300-back-contact-cell-welding-machine-bc-solar-cell-stringer-for-ibc-abc-hpbc-panel-production.html)

### OSLB-1300 BC Cell Stringer: Kwayoyi 1000/sa'a, ±0.10mm

Injin walda tantanin bayan sadarwa na OSLB-1300 daga Ooitech yana ba da aiki fiye da tantanai 1000 a kowace awa don walda igiyar tantanin rana na BC, IBC, ABC, da HPBC.

![Injin Cire Firam ɗin Faifan Rana: Faifai 120 a awa](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774608027244403.webp)

- [** Rachael](./Solar-Panel-Frame-Removal-Machine-High-Efficiency-Automated-Deframing-Equipment.html)
- [** 73646](./Solar-Panel-Frame-Removal-Machine-High-Efficiency-Automated-Deframing-Equipment.html)

### Injin Cire Firam ɗin Faifan Rana: Faifai 120 a awa

Injin cire firam na hasken rana na hydraulic – cire firam ta atomatik don sake amfani da PV module. Ƙarancin karyewa, yana goyan bayan girman panel da yawa.

![PV Backsheet don Solar Modules — TPT, KPK, PVDF](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774518934395196.webp)

- [** Rachael](./Photovoltaic-Backsheet-The-Critical-Protective-Layer-for-Solar-Modules.html)
- [** 13911](./Photovoltaic-Backsheet-The-Critical-Protective-Layer-for-Solar-Modules.html)

### PV Backsheet don Solar Modules — TPT, KPK, PVDF

PV backsheet don solar modules a cikin TPT, KPK, PVDF da kuma bayyanannun nau'ikan: mai jure UV, mai hana wutar lantarki da kuma kariya ta baya mai hana danshi.

![Kayan Gwajin Takaddun Shaida na IEC: 0.1-10kV, 2600mm](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032716200590.webp)

- [** Rachael](./solar-panel-testing-equipment-for-iec-certification-complete-pv-module-test-solutions-by-ooitech.html)
- [** 92497](./solar-panel-testing-equipment-for-iec-certification-complete-pv-module-test-solutions-by-ooitech.html)

### Kayan Gwajin Takaddun Shaida na IEC: 0.1-10kV, 2600mm

Ooitech yana ba da cikakken kewayon kayan gwajin hasken rana don takaddun shaida na IEC61215 da IEC61730, gami da wuraren bincike na gani