# Ƙwayoyin TOPCon a Ƙarƙashin Damp Heat: Me Ya Sa

> Bincike mai zurfi kan dalilin da ya sa rukunin passivation na baya na ƙwayoyin hasken rana na TOPCon ke lalacewa da sauri a ƙarƙashin zafi mai ɗanɗano da gurɓataccen gishirin sodium

![Ƙwayoyin TOPCon a Ƙarƙashin Damp Heat: Me Ya Sa](https://cdn.ooitech.com/static/upload/image/20260717/f468075ae4a8855289bdec6f476ac39b.webp)

- ** 2026-07-17
- ** 293 Ra'ayi
- ** [Blog](./Blog.html)

## Ƙwayoyin TOPCon a Ƙarƙashin Damp Heat: Me Ya Sa

**Amsa mai sauri:** TOPCon ya mamaye yawancin kasuwar silikon crystalline mai inganci, kuma tambayar da ba a warware ba yanzu ba inganci ba ce amma yadda tantanin halitta ke aiki bayan shekaru a fili a ƙarƙashin zafi mai ɗanɗano. Gwajin gaggawa na yau da kullum yana gudana a 85 °C da 85% zafi mai ɗanɗano — DH85 — wanda aka tsara don tura danshi cikin encapsulant da tarin tantanin halitta da sauri fiye da yanayin fili. Tsarin layi yana da mahimmanci a nan: oxide na tunnel kusan 10 nm ƙarƙashin layin polysilicon mai doping yana da sirara sosai cewa sinadarai na mu'amala, ba babban abu ba, ke yanke shawarar aminci. Yanayin zafi na lamination kusan 150 °C da kuma yawan danshi na encapsulant duka suna shiga cikin hanyar lalacewa ɗaya. Ana amfani da kayan aikin bincike a cikin ajin QL200 don bin diddigin abin da fallasa zafi mai ɗanɗano ke yi wa passivation maimakon kawai ko wutar ta ragu.

PV Module Manufacturing · na Jerry, Ooitech

## Gabatarwa

[TOPCon](https://www.ooitech.com/what-is-topcon-solar-cell-a-complete-guide-to-tunnel-oxide-passivated-contact-technology.html) ya mamaye mafi yawan kasuwar c-Si mai inganci, amma amincin filin na dogon lokaci har yanzu manufa ce mai motsi. Wata tabo mai rauni tana ci gaba da bayyana a cikin nazarin zafi-danshi: tarin passivation na baya. Wani bincike na baya-bayan nan (Tong et al., Sol. Energy Mater. Sol. Cells, DOI: 10.1016/j.solmat.2024.113188) ya gano ainihin abin da ke faruwa ba daidai ba lokacin da gishirin sodium ya sauka a saman tantanin halitta kuma ya zauna a ƙarƙashin 85°C/85% RH. Taƙaitaccen bayani — Layer SiNₓ na baya shine wurin da ba shi da ƙarfi, kuma wani siririn fim na ALD AlOₓ yana gyara mafi yawansa.

### Abubuwan da aka gano a gaba

- Layin SiNₓ na baya shine raunin zafi mai danshi. Sodium acetate (CH₃COONa) ya sa ƙarfin buɗe baya (Voc) ya ragu da 5.8% kuma ya tura juriyar jerin (Rₛ) sama da 450%.
- Gishirin sodium suna hanzarta iskar shan iskar oxygen da asarar nitrogen. XPS ya nuna rabon Si/N na baya yana tsalle daga 1.3 zuwa 23, kuma O/N daga 1.6 zuwa 53.
- Shingen ALD Al₂O₃ na 10nm ya yi babban bambanci — asarar PCE a ƙarƙashin gurɓatar CH₃COONa ta ragu daga 16% zuwa 0.4% kawai.
- Kariyar gaba ta fi ƙarfi sosai. Layin AlOₓ/SiOᵧNᵣ mai yawa yana toshe yaduwar sodium, don haka gurɓata a can ta yi asarar PCE 0.87% kawai.
- Abubuwan gurɓata guda biyu suna aiki daban: sodium acetate yana kai hari ga haɗin ƙarfe, yayin da sodium chloride (NaCl) yake iskar shan layin kariya.

## Bayanin Farko

Tambayar asali tana da sauƙi a faɗi, da wuya a amsa: me yasa sel TOPCon ke rasa aiki a ƙarƙashin zafi mai danshi lokacin da gishirin sodium ke kewaye, kuma me yasa kariyar baya ta fi muni (Kyranaki et al., 2022)?

### Inda gibin yake

Yawancin ayyukan da suka gabata sun mayar da hankali kan lalacewar haɗin ƙarfe (Iqbal et al., 2023), amma babu wanda ya yi nazari na tsari kan rushewar sinadarai na layin kariya da kansa. Gaban da baya an gina su daban - gaba shine AlOₓ/SiNₓ/SiOᵧNᵣ, baya shine SiNₓ akan poly-Si mai ƙara - kuma ba a taɓa kwatanta juriyar lalacewarsu kai tsaye ba (Feldmann et al., 2014). A kan haka, gurɓatattun abubuwa guda biyu (CH₃COONa vs. NaCl) an yi tunanin suna da hali ɗaya, amma ba haka suke ba (Li et al., 2021).

Samun wannan daidai yana da mahimmanci ga kuɗi na gaske. Ana siyar da tsire-tsire na PV bisa alƙawarin rayuwa na shekaru 25 (Peters et al., 2021), kuma yanayin gazawar gefen baya da ke bayyana a ƙarƙashin zafi da danshi shine ainihin irin abin da ke cin wannan.

## Hanyar Aiki

An kiyaye tsarin aiki kusa da tsarin samarwa na gaske: sel TOPCon na masana'antu → fesa gishirin sodium a gaba ko baya → haɓaka zafi mai sauri (85°C/85% RH) → siffanta lantarki da sinadarai → gwada shingen ALD AlOₓ → gano hanyar kariya.

### Menon abin da ke nan

A gefen ka'idar, wannan shine bincike na farko da ya nuna asarar nitrogen a cikin SiNₓ na baya shine babban abin da ke haifar da raguwar Voc. A gefen aiki, Layer AlOₓ na 10nm yana aiki akan kayan aikin ALD na masana'antu na yau da kullun kuma yana kashe kusan 0.01% a cikin ingantaccen aiki. Kuma a tsarin, ƙungiyar ta gina gwajin DH na matakin tantanin halitta inda sa'o'i 20 ke wakiltar shekaru da yawa na tsufa a waje (Sen et al., 2023).

Sarkar tunani yana da sauƙin bi: gurɓacewar baya yana haifar da raguwar Voc mai kaifi, wanda ke nuna gazawar kariya kai tsaye. XPS sai ya tabbatar da halayen oxidation na SiNₓ da hanyar sodium da take buɗewa. Ƙara Layer AlOₓ, toshe sodium, kuma hoton PL ya tabbatar da an danne lahani.

## Hanyoyi

### Shirya samfurin

| Abu | Cikakken bayani |
| --- | --- |
| Tsarin tantanin halitta | n-type TOPCon. Gaba: boron-diffused emitter + AlOₓ/SiNₓ/SiOᵧNᵣ, ARC. Baya: SiO₂/phosphorus-doped poly-Si + SiNₓ, ARC |
| Gurɓataccen abu | 0.155 mol/L CH₃COONa ko NaCl bayani, 0.3 g kowace samfurin, fesa gida |
| Shingen ALD | 10nm AlOₓ, an ajiye shi a 150°C (Leadmicro QL200) |
| Damp heat | 85°C/85% RH, 20 hours (ASLi environmental chamber) |

### Yadda aka auna shi

- Ma'aunin I-V (Pmax, Voc, FF, Jsc) ta hanyar tsarin LOANA (pv-tools).
- Ingancin passivation ta hanyar ingantaccen rayuwar mai ɗaukar kaya (τ_eff).
- Kimiyyar saman ta hanyar XPS da SEM-EDS.

## Sakamako da tattaunawa

### Lalacewar lantarki

Gefen baya a fili shine mai rauni. CH₃COONa a baya ya sauke Voc da 5.8%, ya tura Rₛ sama da 450% (Tebur 1), kuma ya yanke ƙarfin PL da 37.3% (Hoto 3a). Haka magani a gaba ya kashe kawai 0.87% PCE. Gishiri ɗaya, sakamako daban-daban sosai dangane da fuskar da ya buga.

### Rushewar sinadarai na passivation

XPS a saman baya ya nuna ɓangaren haɗin Si-O yana tashi sama (Hoto 5b), tare da rabon O/N atomic daga 1.6 a cikin sarrafawa zuwa 53 a cikin rukunin CH₃COONa. Hanyar ita ce asarar nitrogen — zafi mai ɗanɗano yana lalata SiNₓ kuma yana lalata passivation na saman.

### Abin da shingen AlOₓ yake yi

Tare da 10nm ALD AlOₓ a wurin, asarar PCE a ƙarƙashin gurɓataccen CH₃COONa na baya ya faɗi daga 16% zuwa 0.4%, kuma Voc ya tsaya (Fig. 6a). SEM-EDS ya nuna abun ciki na sodium ya ragu da 86% a cikin samfuran AlOₓ (Fig. 6c), kuma PL bai nuna kunna lahani ba (Fig. 6b). Shingen yana yin daidai abin da kuke so — yana hana sodium shiga.

## Ƙarshe

### Babban abubuwan da aka ciro

Layin SiNₓ na baya yana yin hydrolysis kuma yana oxidize a ƙarƙashin zafi mai ɗanɗano da gishirin sodium, wanda ke sa Voc ya ragu kuma Rₛ ya tashi (tare da goyon bayan XPS/EDS, Fig. 4-5). Layin AlOₓ na 10nm yana toshe yaduwar sodium kuma yana kiyaye asarar PCE na DH85 ƙasa da 1% (Fig. 6a). Kuma layin gaba na AlOₓ/SiOᵧNᵣ mai yawa yana da juriya ga lalata, don haka gurɓata a can ba ta da tasiri.

### Dalilin amfaninsa

Shingen AlOₓ na iya shiga kai tsaye cikin samar da TOPCon mai yawa akan kayan aiki kamar Leadmicro QL200. Idan aka duba gaba, haɗa AlOₓ tare da SiNₓ a cikin rufin kwandon gilashi biyu na iya tsawaita rayuwar shuka a yankuna masu ɗanɗano.

## Kadan daga tarihi

- Tsarin TOPCon: oxide tunnel (SiO₂) tare da doped poly-Si lamba mai wucewa, wanda ke yanke sake haɗuwa a karfe (Feldmann et al., 2014).
- ALD: ci gaban nano-film Layer-by-Layer, yana ba da daidaitaccen ɗaukar hoto na nanometer-scale AlOₓ.
- Gwajin DH: 85°C/85% RH tsufa mai sauri don kwaikwayi lalacewar module a yanayin zafi.
- SiNₓ passivation: silicon nitride mai hydrogenated, mai kyau don anti-reflection da surface passivation, amma yana ɗauke da dangling bonds kuma yana hydrolyzes da sauki.

## Nassoshi

- Tong H. et al., Mitigating contaminant-induced degradation in TOPCon solar cells via ALD AlOₓ barrier, DOI: 10.1016/j.solmat.2024.113188
- Feldmann F. et al., Passivated rear contacts for high-efficiency n-type Si solar cells, Solar Energy Materials and Solar Cells 120 (2014) 270–274.
- Li X. et al., Accelerated damp-heat testing of TOPCon cells using NaCl, Solar Energy Materials and Solar Cells 262 (2023) 112554.
- Peters I.M. et al., The value of stability in photovoltaics, Joule 5 (2021) 3137–3153.

## Ra'ayin Ooitech

Abin da ya fi fitowa a nan shi ne yadda yawancin labarin dogaro yake a cikin tarin passivation na baya, ba taken ƙirar tantanin halitta ba. A kan layi na gaske, ƙarin matakin ALD AlOₓ na 10nm shine inshora mai arha don ayyukan yanayi mai ɗanɗano, kuma yana shiga cikin samar da tsarin module ba tare da wahala ba. Muna gina layukan module masu juyawa daga ƙarshe zuwa ƙarshe, don haka muna kallon abubuwan da aka gano kamar wannan a hankali - ƙananan gyare-gyare a sama galibi suna yanke shawarar ko shuka zai tsaya na tsawon shekaru 25. Idan kuna son ƙarin daga bene na masana'anta, tashar YouTube ta Ooitech ([www.youtube.com/ooitech](http://www.youtube.com/ooitech)) tana da daraja a bi ta.

---

##### Tags :

![](/template/ooitech/assets/img/shape/06.png)

![](https://cdn.ooitech.com/runtime/image/w800_h700_fitblur_v2_w800_h700_fitblur_v2_1757399770541443.webp)

### Nemi Farashi

Duk abubuwan da aka ɗora suna da tsaro kuma sirri ne.

## Muna isar da gwanintar da za ka iya amincewa sabis ɗinmu

Kayan aiki kai tsaye daga masana'anta.

![](/template/ooitech/assets/img/icon/money-2.svg)

### Fa'idodin Rage Kuɗi

Muna ba da ƙima ta musamman, muna haɓaka sakamako yayin da muke rage kasafin kuɗi ga abokan ciniki.

![](/template/ooitech/assets/img/icon/staff.svg)

### Ƙungiyar Ƙwarewarmu

Kwararrun ma'aikatanmu sun ƙware a sababbin hanyoyin magance matsaloli da dabarun da aka keɓance.

![](/template/ooitech/assets/img/icon/certified.svg)

### Fiye da Shekaru 15 na Ƙwarewar Masana'antu

Ƙwarewa mai zurfi tana tabbatar da sakamako masu dogaro, masu bin zamani, da tabbatattu don nasara.

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477357667605.webp )

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477724911512.webp)

![](/template/ooitech/assets/img/shape/06.png)

## Abin da Abokin Cinikinmu Ya ce game da mu

Shaidun abokan ciniki sun yaba da zurfin fahimtarmu game da ƙalubalen su, wanda ke haifar da sababbin hanyoyin magance matsaloli da riba mai ƙarfi. Haɗin gwiwa na dogon lokaci—wasu fiye da shekaru goma—suna nuna amincewarsu da gamsuwa. Labaran nasarar su suna motsa mu don ci gaba da wuce tsammanin su. [Ƙara Sani **](#quote-form)

![](/template/ooitech/assets/img/icon/quote.svg)

Mutum mai babban rai. Na gode sosai da ziyarar ku Mista Wu. Na gode sosai da ayyukan da aka bayar wajen shigar da kayan aiki da horar da dalibai na. Mutum mafi kirki kuma ƙwararre a fanninsa.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041716444445.webp)

### Jizzakh Polytechnic Institute

![](/template/ooitech/assets/img/icon/quote.svg)

Na sake godewa sosai don babban taimako na inganta da gyara masana'anta da kuma koya wa ma'aikata yadda ake amfani da injinan

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1757479675272137.webp)

### Mark

BIPV Philippines

![](/template/ooitech/assets/img/icon/quote.svg)

na gode da goyon bayan ƙwararrun ooitech da sabis na bayan lokaci.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1784509010217979.webp)

### Diarra Daga Afirka

![](/template/ooitech/assets/img/icon/quote.svg)

Godiya ga Ooitech don samar da kayan aikin samarwa na atomatik cikakke—shigar da ku da sabis na bayan siyarwa sun yi kyau sosai.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041720921238.webp)

### Amjad

![](/template/ooitech/assets/img/icon/quote.svg)

Godiya ga Ooitech don samar da kayan aikin gwajin ƙwayar hasken rana na BC da suka dace sosai.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1776426122864564.webp)

### KTECH

## Sabbin Kayayyakin Mu

![OTCT-A Mai Gwajin Tantanin Rana: IEC 60904-9, Daraja A](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032746397289.webp)

- [** Rachael](./OTCT-A-Solar-Cell-Tester-High-Precision-Electric-Performance-Testing-Equipment.html)
- [** 16503](./OTCT-A-Solar-Cell-Tester-High-Precision-Electric-Performance-Testing-Equipment.html)

### OTCT-A Mai Gwajin Tantanin Rana: IEC 60904-9, Daraja A

OTCT-A gwajin tantanin hasken rana – fitilar xenon mai darajar A, 16-bit 4-ch samu, IEC60904-9:2020. Ingantaccen ma'aunin lanƙwan IV don mono &amp

![Injin Liƙa Tef Ta Atomatik: Zagayowar 25s, ±2mm](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774350079476146.webp)

- [** Rachael](./automatic-tape-sticking-machine-for-solar-panel-production-line-ooitech.html)
- [** 81708](./automatic-tape-sticking-machine-for-solar-panel-production-line-ooitech.html)

### Injin Liƙa Tef Ta Atomatik: Zagayowar 25s, ±2mm

Injin Liƙa Tef ɗin Ooitech ta atomatik yana liƙa tef ɗin manne a kan igiyoyin ƙwayoyin rana da daidaito da sauri.

![SAW-100A Injin shimfiɗa da haɗa bas: ≤0.3% karyewa](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774349342486074.webp)

- [** Rachael](./automatic-layup-and-bussing-integrated-machine-saw-100a-solar-panel-production-equipment-ooitech.html)
- [** 19633](./automatic-layup-and-bussing-integrated-machine-saw-100a-solar-panel-production-equipment-ooitech.html)

### SAW-100A Injin shimfiɗa da haɗa bas: ≤0.3% karyewa

Injin Haɗa Layup & Bussing ta Atomatik na Ooitech SAW-100A yana ba da layup na igiyar tantani mai inganci da walda busbar ta ƙarshe tare da babban

![Injin Yanke Laser na SC-20P BC Cell](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1772440338787287.webp)

- [** ooitech](./SC-20P-Automatic-Solar-Cell-Laser-Cutting-Machine-High-Precision-BC-Cell-Processing-Equipment.html)
- [** 20725](./SC-20P-Automatic-Solar-Cell-Laser-Cutting-Machine-High-Precision-BC-Cell-Processing-Equipment.html)

### Injin Yanke Laser na SC-20P BC Cell

SC-20P ingantaccen injin yankan laser ne wanda ya dogara da SC-20A, an tsara shi don ƙwayoyin BC. Yana yankan tantanin da takardar kariya lokaci ɗaya zuwa guda 1/2

![DH200-Y Injin Bussing na Atomati: 17s Lokacin Zagayowar](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774348162498246.webp)

- [** Rachael](./automatic-bussing-machine-dh200-y-solar-panel-busbar-soldering-equipment-ooitech.html)
- [** 87779](./automatic-bussing-machine-dh200-y-solar-panel-busbar-soldering-equipment-ooitech.html)

### DH200-Y Injin Bussing na Atomati: 17s Lokacin Zagayowar

Injin Bussing ta atomatik na Ooitech DH200-Y yana ba da aikin walda na busbar na lantarki mai sauri tare da lokacin zagayowar 17s

![Na'urar gwajin EL mai ɗaukuwa: 24MP, tana gano tsagewar 0.2mm](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026051214015103.webp)

- [** ooitech](./portable-hd-el-tester-for-solar-module-inspection.html)
- [** 748](./portable-hd-el-tester-for-solar-module-inspection.html)

### Na'urar gwajin EL mai ɗaukuwa: 24MP, tana gano tsagewar 0.2mm

Mai gwajin EL mai ɗaukuwa mai ma'ana mai girma tare da kyamarar infrared mai da hankali ta atomatik 24MP don gwajin hasken lantarki na tsarin hasken rana