# UVID a cikin Kwayoyin Rana na TOPCon: Gwajin IV Mara Tuntuɓa

> Nazari kan lalacewar da UV ke haifarwa (UVID) a cikin ƙwayoyin hasken rana na TOPCon ta amfani da gwajin IV mara tuntuɓa, ToF-SIMS da binciken zurfin XPS don bayyana hydrogen da

![UVID a cikin Kwayoyin Rana na TOPCon: Gwajin IV Mara Tuntuɓa](https://cdn.ooitech.com/static/upload/image/20260804/17aeb9818f648b0a8226d34423b2a293.webp)

- ** Jerry
- ** 2026-08-04
- ** 290 Views
- ** [Blog](./Blog.html)

## UVID a cikin Kwayoyin Rana na TOPCon: Gwajin IV Mara Tuntuɓa

**Amsa mai sauri:** Binciken UVID akan sel TOPCon yana amfani da gwajin IV mara tuntuɓa saboda lalacewar tana tasowa ne a tsawon lokacin fallasa kuma ma'aunin da kansa bai kamata ya canza abin da ake aunawa ba. Tuntuɓar sel don ɗaukar karatun IV yana lalata ƙarfen ɗan kaɗan, wanda zai taru a kan maimaita ma'auni kuma ya sa layin lalacewar ba a iya karantawa. Hanyoyin marasa tuntuɓa suna karanta sel ta hanyar gani maimakon, don haka ana iya bin diddigin samfurin ɗaya ta jerin fallasar UV. Yanayin damuwa a cikin wannan aikin suna amfani da fallasar UV a 60 °C a cikin jeri na bakan 120 nm, 400 nm da 500 nm, tare da samfuran da aka sanya wa UV60. Amfanin TOPCon akan gine-ginen da suka gabata ya fito ne daga passivation na samansa da zaɓin mai ɗauka, kuma UVID shine tsarin da ke kai hari daidai waɗannan kaddarorin, wanda shine dalilin da yasa ake bin diddiginsa daban da aikin damp-heat.

PV Module Manufacturing · na Jerry, Ooitech

## Gabatarwa

[TOPCon](https://www.ooitech.com/what-is-topcon-solar-cell-a-complete-guide-to-tunnel-oxide-passivated-contact-technology.html) Kwayoyin hasken rana a yanzu sun mamaye kasuwar PV saboda ƙarfin passivation na saman da lambobin da ke zaɓar mai ɗauka. Amma aiki a waje yana fallasa wata muhimmiyar rauni: lalacewar da UV ke haifarwa, ko UVID. Bayan hasken UV60, inganci yana raguwa da kusan 6.72%.

Yawancin ayyukan da suka gabata sun zargi UVID da manyan photons masu ƙarfi da ke karya Si–H bonds da sakin hydrogen kyauta. Wannan ɓangare ne kawai na labarin. Bakan UV na hasken rana ya kai faɗin kewayon makamashi na 3.1–4.43 eV, don haka mu'amalarsa da saman gaba ya wuce hanyar karyewar Si–H guda ɗaya. Kuma gaban Al₂O₃ / SiNₓ yana da rauni sosai a kan UV fiye da gefen baya.

Gwajin IV mara lamba yana taimakawa sosai a nan. Ba ya lalata kayan, ba ya amfani da kayan amfani, yana aiki cikin sauri a millisecond, yana aiki da BC da kuma ƙirar da ba ta da busbar, kuma yana ɗaukar sigogin IV, EQE da PL a lokaci guda.

Wannan binciken yana amfani da ToF-SIMS da XPS mai zurfin bayanai don bin diddigin rarraba abubuwa da canje-canjen haɗin sinadarai a cikin Al₂O₃ / SiNₓ kafin da bayan UV60. Sakamakon: Rushewar haɗin N–H shine tushen hydrogen na biyu tare da Si–H. Haɗin Al–O a cikin amorphous Al₂O₃ yana rushewa ta hanyar UV kuma yana haifar da ɗimbin guraben oxygen. Hanyoyin hydrogen da oxygen suna taruwa kuma suna ƙara lalata sake haɗuwa a saman, suna ba da kyakkyawar hanya don inganta amincin passivation.

## Hanyar Gwaji

(a) Tsarin tsarin hasken rana na TOPCon (b) samfurin tsarin gaba mai ma'ana (c) samfurin tsarin baya mai ma'ana

An shirya samfuran tsarin gaba mai ma'ana (SiNₓ/Al₂O₃/n-Si/Al₂O₃/SiNₓ) da samfuran tsarin baya mai ma'ana (tare da SiOₓ/n⁺-poly-Si). An gudanar da tsufa na UV a matakin module. Babban tushen haske shine UV-A tare da kusan 11% UV-B, a ƙarƙashin 60°C da 30% zafi.

Ƙarfin hasken UV mai haske

## Tsarin Gaba vs Baya: Kwatanta Juriyar UV

Canje-canje a (a) τeff a ƙaddarar allurar mai ɗaukar nauyi na 1×10¹⁵ cm⁻³, (b) iVoc, da (c) J₀ na gefe ɗaya don samfuran tsarin gaba da baya masu daidaitawa yayin fallasa UV

Tsarin baya mai daidaitawa da kyar ya lalace bayan fallasa UV na 60 kWh·m⁻². Tsarin poly-Si mai kauri 120 nm yana sha kusan duk hasken UV kuma yana ba da kariya mai inganci.

Tsarin gaba ya ba da labari daban. τeff ya ragu daga 2895.6 μs zuwa 1552.8 μs. iVoc ya faɗi daga 735.5 mV zuwa 715.2 mV. J₀ na gefe ɗaya ya tashi zuwa 18.4 fA·cm⁻², kusan sau uku na ƙimar farko. Kariyar Al₂O₃ / SiNₓ ta lalace sosai.

## Juyin Halittar Sinadaran

Zurfin bayanan ƙarfi na (a) hydrogen da (b) oxygen a cikin samfurin tsarin gaba mai daidaitawa da aka goge kafin da bayan UV60, wanda ToF-SIMS ya auna

ToF-SIMS ya nuna yawan hydrogen yana ƙaruwa a fili bayan fallasa UV, musamman a cikin Layer SiNₓ. N 1s XPS zurfin bayanan ya nuna cewa a mahadar SiNₓ / Al₂O₃, rabon haɗin N–H ya faɗi daga 9.64% zuwa 5.97%. Don haka karya haɗin N–H shine tushen hydrogen na biyu bayan Si–H. Hydrogen ɗin da aka saki yana yaduwa zuwa yankin saman SiNₓ kuma yana sake haɗuwa da silicon a can, wanda shine dalilin da yasa rabon N–H a zahiri ke ƙaruwa kusa da wannan saman.

Oxygen yana ba da labari mai mahimmanci daidai. Oxygen a cikin Layer Al₂O₃ ya ragu kadan, yayin da oxygen a interfaces SiNₓ/Al₂O₃ da Al₂O₃/Si ya karu. Wannan yana nuna cewa Al–O bonds suna karyewa kuma free oxygen yana ƙaura zuwa waje. Ƙarfin Al–O bond a cikin crystal mai kyau kusan 5.3 eV ne. Amma a cikin amorphous Al₂O₃, aluminum ions da ba su da cikakken coordination da oxygen vacancies suna kama electrons kuma su zama masu caji mara kyau, suna rage activation energy don karyewar Al–O bond da ke kusa zuwa kusan 2.4 eV. Wannan yana nufin hasken UV na 400 nm (3.1 eV) ya isa ya karya su.

N 1s depth-profiling XPS spectra a interfaces daban-daban na Layer Al₂O₃/SiNₓ kafin da bayan UV60, tare da fitted curves don N–Si (397.5 eV) da N–H (399.5 eV) bonds

O 1s XPS yana nuna lattice oxygen (OI) yana canzawa zuwa oxygen vacancies (OII). A cikin Al 2p spectra, rabon Al₂O₃ ya fadi daga 69.99% zuwa 60.36% yayin da Al–OH ya tashi daga 30.01% zuwa 39.64%. A cikin Si 2p spectra, Si²⁺ ya karu yayin da silicon mai girma valence ya ragu. Electrons da aka saki lokacin da oxygen vacancies suka samu suna rage silicon daga yanayin oxidation mafi girma. Gaba daya, waɗannan canje-canje a cikin bonding na oxygen, aluminum da silicon suna nuna cewa ingancin fim ɗin Al₂O₃ ya riga ya lalace.

## Rashin Ayyukan Lantarki

EQE da reflectance curves na TOPCon solar cell kafin da bayan UV60

Canji a juriyar tuntuɓar gaba na tantanin rana na TOPCon yayin bayyanar UV60

Reflectance ya kasance ba canzawa bayan UV60. EQE ya nuna raguwa matsakaici a yankin gajeren zango ƙasa da 500 nm, daidai da ƙarar sake haɗuwa a saman gaba. Juriyar tuntuɓar gaba ta haura kusan layi da adadin UV, ta kai 4.1 mΩ·cm², kusan sau 8.6 mafi girma. Dalili: hydrogen da oxygen kyauta da aka samar a cikin layin kariya suna yaduwa zuwa ƙarshen lantarki kuma suna shiga cikin halayen redox. UV kuma yana canza kwayoyin ruwa a saman azurfa zuwa radicals hydroxyl, kuma tare suna lalata ƙarfen lantarki.

Ƙimar raguwar aikin lantarki yayin bayyanar UV60: (a) Voc (b) Jsc (c) FF (d) Eff

Voc ya ragu 3.46% dangantaka, wanda aka motsa ta hanyar lalacewar kariyar saman gaba da haɓakar J₀. FF ya faɗi 2.82%, wanda aka motsa ta hanyar mafi girman juriyar tuntuɓar gaba. Jsc kawai ya ragu 0.64%, tunda asarar EQE a gajeren zango ta iyakance. Ƙarshen asarar ingancin juyar da haske zuwa wutar lantarki ya kai 6.72%.

## Ƙarshe

Tsarin SiNₓ/Al₂O₃ na gaba na sel TOPCon yana da rauni sosai a ƙarƙashin UV fiye da tsarin baya. A ƙarƙashin UV, haɗin Si–H da N–H suna karyewa a jere kuma suna sakin hydrogen kyauta. Haɗin Al–O a cikin amorphous Al₂O₃ yana karyewa a ƙarƙashin UV, yana sakin oxygen kyauta kuma yana haifar da ɗimbin guraben oxygen. Al₂O₃ yana juyawa zuwa Al–OH kuma ƙimar silicon tana canzawa. Waɗannan hanyoyin lalacewa guda biyu, hydrogen da oxygen, suna taruwa kuma suna ƙara tsananta sake haɗuwa a saman. Ƙara haɓakar juriyar tuntuɓar gaba, sakamakon shine asarar inganci 6.72%. Aikin yana ba da cikakken bayani mai amfani don fahimtar UVID na TOPCon da kuma inganta dogaro na dogon lokaci na yadudduka na kariya.

## Ra'ayin Ooitech

UVID yana ci gaba da tabbatar da cewa tsarin gaba shine inda ake gwada dogaro da gaske, don haka yadda kuke ginawa da sarrafa ajiyar SiNₓ/Al₂O₃ da rufewa akan layin module yana da mahimmanci kamar girke-girke na cell. A kan layukan mu na turnkey TOPCon da PERC module muna ganin wannan darasi yana faruwa a kan layup, lamination da gefen EL, ƙananan zaɓin tsari suna yanke shawarar ko allunan suna tsayawa a waje tsawon shekaru. Idan kuna son ƙarin ra'ayoyi na hannu daga filin masana'anta, tashar YouTube ta Ooitech a [www.youtube.com/ooitech](http://www.youtube.com/ooitech) tana da daraja a bi.

Masu alaƙa: [TOPCon UVID da r-UVID / ir-UVID rabuwa](https://www.ooitech.com/topcon-uvid-reversible-and-irreversible-uv-degradation.html) yana bayyana dalilin da ya sa wannan module ɗin yake karantawa daban-daban dangane da lokacin da aka ɗauki ma'aunin.

## Ƙarin karatu da bayanan baya

Kayan tunani na jama'a kan wannan batu, wanda ƙungiyoyin da ke kula da taswirar fasahar masana'antar da bayanan kasuwa suka wallafa:

- [Fraunhofer ISE — Rahoton Photovoltaics](https://www.ise.fraunhofer.de/en/publications/studies/photovoltaics-report.html)
- [Ma'aikatar Makamashi ta Amurka — Photovoltaics](https://www.energy.gov/eere/solar/photovoltaics)
- [VDMA — Taswirar Fasahar Ƙasa da Ƙasa don Photovoltaic (ITRPV)](https://www.vdma.org/international-technology-roadmap-photovoltaic)

---

##### Tags :

![](/template/ooitech/assets/img/shape/06.png)

![](https://cdn.ooitech.com/runtime/image/w800_h700_fitblur_v2_w800_h700_fitblur_v2_1757399770541443.webp)

### Nemi Farashi

Duk abubuwan da aka ɗora suna da tsaro kuma sirri ne.

## Muna isar da gwanintar da za ka iya amincewa sabis ɗinmu

Kayan aiki kai tsaye daga masana'anta.

![](/template/ooitech/assets/img/icon/money-2.svg)

### Fa'idodin Rage Kuɗi

Muna ba da ƙima ta musamman, muna haɓaka sakamako yayin da muke rage kasafin kuɗi ga abokan ciniki.

![](/template/ooitech/assets/img/icon/staff.svg)

### Ƙungiyar Ƙwarewarmu

Kwararrun ma'aikatanmu sun ƙware a sababbin hanyoyin magance matsaloli da dabarun da aka keɓance.

![](/template/ooitech/assets/img/icon/certified.svg)

### Fiye da Shekaru 15 na Ƙwarewar Masana'antu

Ƙwarewa mai zurfi tana tabbatar da sakamako masu dogaro, masu bin zamani, da tabbatattu don nasara.

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477357667605.webp )

![](https://cdn.ooitech.com/static/upload/image/20250910/1757477724911512.webp)

![](/template/ooitech/assets/img/shape/06.png)

## Abin da Abokin Cinikinmu Ya ce game da mu

Shaidun abokan ciniki sun yaba da zurfin fahimtarmu game da ƙalubalen su, wanda ke haifar da sababbin hanyoyin magance matsaloli da riba mai ƙarfi. Haɗin gwiwa na dogon lokaci—wasu fiye da shekaru goma—suna nuna amincewarsu da gamsuwa. Labaran nasarar su suna motsa mu don ci gaba da wuce tsammanin su. [Ƙara Sani **](#quote-form)

![](/template/ooitech/assets/img/icon/quote.svg)

na gode da goyon bayan ƙwararrun ooitech da sabis na bayan lokaci.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1784509010217979.webp)

### Diarra Daga Afirka

![](/template/ooitech/assets/img/icon/quote.svg)

Mutum mai babban rai. Na gode sosai da ziyarar ku Mista Wu. Na gode sosai da ayyukan da aka bayar wajen shigar da kayan aiki da horar da dalibai na. Mutum mafi kirki kuma ƙwararre a fanninsa.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041716444445.webp)

### Jizzakh Polytechnic Institute

![](/template/ooitech/assets/img/icon/quote.svg)

Godiya ga Ooitech don samar da kayan aikin samarwa na atomatik cikakke—shigar da ku da sabis na bayan siyarwa sun yi kyau sosai.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026041720921238.webp)

### Amjad

![](/template/ooitech/assets/img/icon/quote.svg)

Na sake godewa sosai don babban taimako na inganta da gyara masana'anta da kuma koya wa ma'aikata yadda ake amfani da injinan

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1757479675272137.webp)

### Mark

BIPV Philippines

![](/template/ooitech/assets/img/icon/quote.svg)

Godiya ga Ooitech don samar da kayan aikin gwajin ƙwayar hasken rana na BC da suka dace sosai.

![](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1776426122864564.webp)

### KTECH

## Sabbin Kayayyakin Mu

![SAW-100A Injin shimfiɗa da haɗa bas: ≤0.3% karyewa](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774349342486074.webp)

- [** Rachael](./automatic-layup-and-bussing-integrated-machine-saw-100a-solar-panel-production-equipment-ooitech.html)
- [** 19728](./automatic-layup-and-bussing-integrated-machine-saw-100a-solar-panel-production-equipment-ooitech.html)

### SAW-100A Injin shimfiɗa da haɗa bas: ≤0.3% karyewa

Injin Haɗa Layup & Bussing ta Atomatik na Ooitech SAW-100A yana ba da layup na igiyar tantani mai inganci da walda busbar ta ƙarshe tare da babban

![OTCY-2754DD Mai Laminator na BIPV: Ɗaki Biyu, Layer Ɗaya](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774438298752758.webp)

- [** Rachael](./OTCY-2754DD-Single-Layer-Double-Chamber-Automatic-BIPV-Laminator-High-Performance-Solar-Module-Produ.html)
- [** 63434](./OTCY-2754DD-Single-Layer-Double-Chamber-Automatic-BIPV-Laminator-High-Performance-Solar-Module-Produ.html)

### OTCY-2754DD Mai Laminator na BIPV: Ɗaki Biyu, Layer Ɗaya

Cikakken katalogin Ooitech na laminator na hasken rana: samfura 10, kwatancen fasaha, bayanin tsarin, kula da aminci

![Ribbon PV na Yanayin Zafi Ƙasa da Flux don igiyoyin hasken rana](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032717287347.webp)

- [** Rachael](./Solar-Panel-Soldering-Ribbon-and-Flux-Essential-Components-for-PV-Module-Manufacturing.html)
- [** 21211](./Solar-Panel-Soldering-Ribbon-and-Flux-Essential-Components-for-PV-Module-Manufacturing.html)

### Ribbon PV na Yanayin Zafi Ƙasa da Flux don igiyoyin hasken rana

Ribbon na PV da flux don haɗa ƙwayoyin hasken rana: ribbon na solder mai zafin ƙasa a cikin tagulla mai tsabta da aka lulluɓe da tin, yana goyan bayan layukan MBB da rabin yanke.

![CHT9980A Mai Gwajin Tsaro na PV: 8kV, 0.001kV Ƙuduri](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_2026032763823477.jpg)

- [** Rachael](./cht9980a-cht9981a-pv-safety-comprehensive-tester-solar-panel-hipot-insulation-ground-continuity-tester.html)
- [** 84014](./cht9980a-cht9981a-pv-safety-comprehensive-tester-solar-panel-hipot-insulation-ground-continuity-tester.html)

### CHT9980A Mai Gwajin Tsaro na PV: 8kV, 0.001kV Ƙuduri

CHT9980A/CHT9981A PV Safety Comprehensive Tester kayan aiki ne mai inganci guda 3 da suka haɗa da jurewar wutar lantarki ta DC, juriyar rufi

![Na'urar Ajiye Tantanin Halitta ta Robot HS-PBR: 5s/Zare, ±0.3mm](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774338062497258.webp)

- [** Rachael](./robot-string-cell-layup-machine-hs-pbr-automated-solar-module-layup-system-ooitech.html)
- [** 67727](./robot-string-cell-layup-machine-hs-pbr-automated-solar-module-layup-system-ooitech.html)

### Na'urar Ajiye Tantanin Halitta ta Robot HS-PBR: 5s/Zare, ±0.3mm

Injin Ooitech HS-PBR Robot String Cell Layup yana samar da ingantaccen tsarin tantancewar igiya ta atomatik tare da daidaito ±0.3mm da lokacin zagaye ≤5s kowace

![Injin Liƙa Tef Ta Atomatik: Zagayowar 25s, ±2mm](https://cdn.ooitech.com/runtime/image/w800_h600_fitblur_v2_1774350079476146.webp)

- [** Rachael](./automatic-tape-sticking-machine-for-solar-panel-production-line-ooitech.html)
- [** 81810](./automatic-tape-sticking-machine-for-solar-panel-production-line-ooitech.html)

### Injin Liƙa Tef Ta Atomatik: Zagayowar 25s, ±2mm

Injin Liƙa Tef ɗin Ooitech ta atomatik yana liƙa tef ɗin manne a kan igiyoyin ƙwayoyin rana da daidaito da sauri.