Alhakin edita na wannan labarin yana hannun Wuhan Ooi Photoelectric Technology Co., Ltd. An rubuta kuma an duba shi daga ƙungiyar edita ta Ooitech. Duba manufar edita don yadda muke rubutu, inda ake amfani da kayan aikin AI, da yadda za a nemi gyara.
Kamfanin Hasken Rana na Aljeriya Ya Sayi 3A Grade IV Tester
Teburin Abubuwan Ciki
Kamfanin PV na Aljeriya Ya Sami Na'urar Gwajin IV na Aji 3A da Dakin Gwajin Muhalli daga Ooitech
A cikin 2017, wani kamfanin photovoltaic da ke Aljeriya ya ba da oda ga Ooitech don kayan gwajin hasken rana na ci gaba, gami da na'urar gwajin IV na 3A da kuma dakin gwajin yanayi na zafi-danshi-daskare. Sayen wani bangare ne na kokarin kamfanin na gina ingantaccen kula da inganci da gwajin dogaro don samar da hasken rana.

Na'urar Gwajin IV na 3A
Darajar 3A na'urar kwaikwayo ta hasken rana da na'urar gwajin IV an ƙera su don auna aikin lantarki na fafutukan rana a ƙarƙashin yanayin gwaji na yau da kullun (STC). Rarraba "3A" yana nufin kayan aikin sun cika mafi girman ƙa'idoji a daidaiton bakan, daidaiton sarari, da kwanciyar hankali na lokaci bisa ga IEC 60904-9. Wannan yana ba wa masana'anta na Aljeriya damar auna daidai ƙarfin fitarwa, lanƙwanin ƙarfin lantarki, da ingancin kowane module kafin jigilar su.

Dakin Gwajin Yanayi
Ɗakin gwajin muhalli yana tallafawa zagayowar zafin jiki, fallasa zafi, da gwajin daskarewa bisa ga ƙa'idojin IEC 61215. Waɗannan gwaje-gwajen suna kwaikwayon shekaru na yanayin yanayi na ainihi cikin ɗan gajeren lokaci, suna taimakawa gano lahani masu yuwuwa kamar rarrabuwa, fashewar tantanin halitta, ko akwatin haɗin wutar lantarki kafin samfuran su isa filin.
Wannan isar da kayan aiki yana nuna karuwar buƙatar kayan aikin gwajin hasken rana a Arewacin Afirka yayin da yankin ke ci gaba da faɗaɗa ƙarfin sabunta makamashi.