Alhakin edita na wannan labarin yana hannun Wuhan Ooi Photoelectric Technology Co., Ltd. An rubuta kuma an duba shi daga ƙungiyar edita ta Ooitech. Duba manufar edita don yadda muke rubutu, inda ake amfani da kayan aikin AI, da yadda za a nemi gyara.

BC Stringing Warp: Ƙarshen Biyu Lanƙwasa, Levers Biyar don Gyara Shi

Amsa mai sauri: Kwayoyin back-contact suna barin stringer a kwance a tsakiya kuma a ɗaga a ƙarshen biyu saboda zafi yana zuwa gefe ɗaya kawai kuma ba a riƙe ƙarshen ba. Layukan da ba a inganta ba suna gudanar da 1.0–1.5 mm na warp na ƙarshe, kuma ɓangarori masu tsanani sun wuce 2 mm a kan haƙurin layup na ±0.5 mm. Maganin ba ƙaramin ƙarfe mai sanyaya ba ne: hanyoyi biyar ne da aka saita tare — preheat na gaba, tashin hankali na yankin ƙarshe, binning na warp mai shigowa, riƙewa mai faɗin cikakke, da girke-girke daban-daban na kowane wafer da ƙayyadaddun ribbon.

Stringer da ke walda kwayoyin back-contact da mugun aiki ba yawanci yakan gaza da ƙarfi ba. Kwayoyin suna fitowa da tsakiya an matse shi a kwance a kan platen kuma ƙarshen biyu a tsaye kaɗan, kamar yadda takardar takarda ke ɗagawa lokacin da ka riƙe tsakiyarta kawai. Haɗin yana kama da kyau a ƙarƙashin microscope. Lalacewar tana bayyana tashoshi biyu daga baya, lokacin da robot ɗin layup ya kasa samun gefen pad da yake tsammani.

Ma'aikata suna kiransa jirgin ruwa. Siffar ta isa a gane ta daga hoto: ƙasa a tsakiya, tsayi a ƙarshen, tare da yawancin ɗagawa a kusan kashi biyar na waje na tantanin halitta a alkiblar ciyarwa. Wannan labarin game da wannan siffar — abin da ke haifar da ita, abin da take kashewa a ƙasa, da saitunan biyar da ke dawo da ita ƙarƙashin iko. Idan kana son ilimin kimiyyar kayan da ke bayanin dalilin da yasa tantanin halitta mai tuntuɓar baya ke lanƙwasa kwata-kwata, wannan yana an rufe shi daban; a nan muna kan layi.

Siffar ita ce ganewar asali

Lanƙwasawa bayan ɗaurewa yana da halaye uku da za a iya aunawa, kowanne yana nuni ga wani dalili daban. Auna su kafin ka canza wani abu, domin lambar da aka ɗauka bayan canjin siga ba ta gaya maka komai game da inda ka fara ba.

Abin da kuke ganiAbin da yawanci yake nufiAbin da za a rubuta
Ƙarshen sama, tsakiya lebur, daidaitacceRashin daidaiton zafi tare da ƙarshen da ba a takura — alamar ɗaurewa ta gargajiyaLanƙwasawa a kashi biyar na waje na kowane ƙarshe, fuskoki biyu
Ɗaya ƙarshen ya fi ɗayan tsayiRashin daidaito na tashin hankali ko platen da ba ta daidaita a faɗin fadinWanne ƙarshen, da ko yana motsi da canje-canjen reel ɗin ribbon
Lanƙwasa gefe maimakon lanƙwasa ƙarsheDamuwar wafer mai shigowa, ba walda baLanƙwasawar sel ɗin nan kafin su shiga injin
Lanƙwasawa da ke girma bayan kwana ɗayaDamuwa saura har yanzu tana sassautawa — a sake auna a sa'o'i 24Lanƙwasawa a sa'o'i 0, 1 da 24 akan samfurin guda

Lambobin da suka fi muhimmanci cikakke ne, ba dangi ba. Layi ba tare da keɓaɓɓen ingantawa ba yawanci yana bayar da 1.0–1.5 mm matsakaicin lanƙwasawa bayan stringing, tare da gungun marasa kyau da suka wuce 2 mm. Tashar layup da ke karɓar waɗannan strings tana buƙatar sanya su cikin ±0.5 mm. Duk abin da ya wuce wannan haƙuri ba batun kwalliya ba ne; kuskuren sanyawa ne da ke jira ya faru, kuma string ɗin ba dole ba ne ya zama a bayyane ya lanƙwasa don ya gaza.

Wata bayani mai amfani kan awo: bayyana warp a matsayin tsayi bisa wani tazara da aka ayyana, kuma ka faɗi wace tazara ce. Lamba ba tare da tsawon ma'auni ba ba za a iya kwatanta ta tsakanin masana'antu ba, kuma yawancin sabani kan ko wani rukuni na “cikin ka'ida” ne da gaske sabani ne kan yadda aka auna shi.

Me ya sa ake auna ƙarshen ba tsakiyar ba

Ana kuma dumama tantanin da ke da lamba ta gaba daga baya, amma gaban yana ɗauke da cikakken grid na ƙarfe. Zafi yana bazuwa a fuskoki biyu, ɓangarorin biyu suna faɗaɗa kusa da juna, kuma sauran damuwa bayan sanyaya kaɗan ne har wafer mai 150 µm yana shanye shi. Tantanin da ke da lamba ta baya ba shi da ƙarfe a gaba. Duk zafin yana shiga ta baya, gaban yana zama mai sanyi, kuma yayin sanyaya baya yana raguwa fiye da gaba. Tantanin yana son lanƙwasa, kuma yana lanƙwasa zuwa gaba.

Inda lanƙwasawa ke bayyana shi ne na'urar riƙe ke yanke shawara, ba ƙarfe ba. Faranti na al'ada yana riƙe tantanin kusa da tsakiyarsa. Tsakiyar ba za ta iya motsi ba, don haka ana tura damuwa waje kuma ana sakin ta a ƙarshen, waɗanda babu abin da ke riƙe su. Sakamakon ba lanƙwasa iri ɗaya ba ne amma hinge a kowane ƙarshen — daidai siffar jirgin ruwa da ma'aikata ke bayarwa, kuma daidai yankin da sanya busbar ko gefen pad ya fi rauni a tsarin lamba ta baya.

Wannan kuma shine dalilin da yasa yawan sanyaya yake da mahimmanci kamar mafi girman zafin jiki. Saukin faduwa yana kulle rashin daidaituwa kafin tantanin ya sami damar shakatawa; jinkirin hawa yana barin ribbon da solder su daidaita wani ɓangare na shi. Layi biyu da suke gudana daidai da mafi girman zafi akan yanayin sanyaya daban-daban zasu bayar da rahoton karkacewa daban, kuma babu wanda yake ƙarya.

Abubuwa huɗu masu ninkawa waɗanda suke juya ƙaramin rashin daidaituwa zuwa lahani

Rashin daidaiton zafi shine tushen asali, amma shi kaɗai yana haifar da karkacewa wanda tashar ajiya zata iya jurewa. Abin da yake juya shi zuwa 2 mm shine jerin abubuwa masu ninkawa waɗanda suke taruwa.

Ƙarfin ribbon da aka aro daga layin busbar

Moduloli na baya-baya suna aiki da ribbon mai kyau a cikin kewayon 0.15–0.22 mm, kuma siririn ribbon yana ƙara ƙarfin duk abin da aka ba shi. Ribbon yana faɗaɗawa yayin zafi kuma yana raguwa yayin sanyaya; idan an saita ƙarfin da yawa, wannan raguwar tana jan gefen tantanin maimakon daidaita tsiri. Sassan ƙarshen kuma suna ɗauke da tattara zafin haɗin busbar, don haka suna raguwa fiye da tsakiya. Kwafin girke-girke na ƙarfin gaba-gaba akan samfurin baya-baya shine mafi yawan sanadin ɗan adam na karkacewar ƙarshen da ya wuce gona da iri — girke-girken yana kama da mai tsauri saboda ya yi aiki akan samfurin da ya gabata.

Wafer mai rabin taurin wanda aka rubuta girke-girken don shi

Kwayoyin da ke da lamba ta baya suna tsayawa a 100–120 µm, yayin da na gaba na yau da kullum ke kusan 150 µm. Taurin yana raguwa da sauri fiye da kauri, don haka karfin lankwasawa iri daya yana haifar da karkatawa mai yawa. Girke-girken da aka daidaita akan silicon na 150 µm ba kuskure kadan ba ne akan silicon na 110 µm; tsari ne daban.

Damuwar da ta zo tare da kwayar

Kwayoyin suna barin layin kwayoyin da damuwa ta ciki da ta rage daga toshewa da sanya karfe. Sanya gishirin narkakke abu ne na sakin damuwa: ana dumama kwayar, damuwar tana dan sassautuwa, kuma saboda karshen suna da 'yanci sakin yana bayyana a matsayin nakasawa. Kimantawar masana'antu sun nuna damuwar da ke shigowa tana da fiye da kashi 30% na jimillar gudummawar karkatawa, wanda shine dalilin da yasa layin da ke gyara injin walda kawai zai iya tsayawa sama da manufa.

Faranti da ke rike tsakiya kawai

Vacuum na tsakiya kawai shine na yau da kullum saboda ya isa ga kwayoyin lamba ta gaba. Akan kwayar lamba ta baya siririya yana juya damuwa mai daidaito zuwa madaidaicin kofa. Wannan takurawar inji ce ba ta girke-girke ba, kuma ita ce hanyar da aka fi barin ba a taba ba saboda tana kama da kashe kudi na babban jari maimakon aikin tsari.

Abin da karkatawa ke kashewa bayan ta bar injin walda

Ƙarshen yaƙi ba lahani ne na tasha ɗaya ba; yana tafiya. Igiyar tana isa tashar busbar da ƙarshenta a ɗagawa, kuma haɗin busbar — wanda ya riga ya zama haɗin da ba shi da afuwa a cikin module ɗin — ana walda shi a kan rata da ta canza bayan an saita injin ɗin. Wannan hanya ɗaya ce zuwa ga haɗin sanyi da haɗin da aka ɗaga waɗanda ke bayyana daga baya a matsayin tsagewar lamination.

A lokacin shimfiɗawa, tsarin hangen nesa da ke neman gefen pad ko fiducial yana samun saman a wani tsayi daban kuma, mafi muhimmanci, a wani kusurwa daban. Faɗakarwar karkatar da wuri tana biyo baya, kuma matakan juyawa da canja wuri suna riƙe da igiya mai lanƙwasa da kofin tsotsa wanda kawai yake taɓa wani ɓangare nata. Kowanne daga cikin waɗannan matakan yana ƙara haɗarin karyewa wanda ake danganta shi da sarrafawa maimakon da injin igiyar da ya haifar da shi.

A lokacin lamination damuwa yana saki maimakon ƙarawa — ana matse module ɗin ya kwanta kuma a riƙe shi da zafi na mintuna, kuma ragowar damuwar ko dai tana sakin jiki cikin encapsulant ko tana mai da hankali a haɗi. Idan ta mai da hankali, sakamakon shine microcrack wanda ba ya bayyana a hoton EL na bayan igiya. Shi ya sa layi zai iya wuce gwajin EL ɗinsa kuma har yanzu ya aika da module mai fashewar tantanin halitta.

Lokacin da ake lamination na igiyoyi tare da warp mai saura har zuwa 1.5 mm, muna tsara matsin ɗakin da zafin platen a hankali don encapsulant ya gudana a kusa da haɗin gwiwa kafin cikakken nauyin inji ya matse sel ɗin a kwance.

Kuɗin da ake kashewa na dogon lokaci shine gajiyawa. Haɗin gwiwa da ke ƙarƙashin damuwa mai saura yana juyawa ta cikin kewayon damuwa mai faɗi fiye da wanda ba shi da damuwa, don haka yakan kai ga lalacewa da wuri a cikin zagayowar zafi. Kuna biyan kuɗin warp sau biyu: sau ɗaya a cikin amfanin ranar, kuma sake a cikin bayanan filin shekaru huɗu bayan haka.

Sashe na giciye da ke nuna shigar zafi na gefen baya yana sa baya ya yi ƙanƙanta fiye da gaba, tare da tsakiya a riƙe kuma duka ƙarshen a kwance don ɗagawa

Zafin gefen baya, gaba mai sanyi, da ƙarshen biyu da ba a riƙe: damuwar tana da wuri ɗaya kawai da za ta je.

Hanyoyi biyar, da saitunan da suka fi muhimmanci akan kowanne

Sarrafa warp matsala ce ta tsarin, kuma daidaita hanyar ɗaya da kyau yayin barin huɗu kawai yana haifar da ɗan ƙaramin ci gaba da sabon lahani. Biyar ɗin da ke ƙasa an jera su bisa yawan canjin da suke yi ga sakamako a kowane mako na ƙoƙarin injiniya, ba bisa farashi ba.

LeverSaitin da ya fi muhimmanciAbin da za a tabbatar
Filin zafiDumama ta gaba 80–100 °C, bambanci tsakanin gaba da baya ƙasa da 50 °C, ƙarfin yankin ƙarshe 10–15% ƙasa da tsakiyaAn auna zafin gaba da baya a kan tantanin halitta ɗaya, ba saitin da aka sa ba
Ƙarfin jaƘarfin ja mai madauki na yau da kullum, sassan ƙarshe 20–30% ƙasa, izinin raguwar 0.5–1 mm a ƙarshenƘarfin ja a kan reel, a sashin ƙarshe, da kuma bayan canjin reel
Kayan shigowaCikakken bincike na karkacewa da rabawa, girke-girke na musamman ga kowane rukuni, dumama kafin annealing a 100–120 °C na kusan 30 sKarkacewa kafin da bayan annealing a kan rukuni ɗaya
RiƙewaDandali mai laushi mai faɗin cikakke tare da vacuum na gefe, riƙe 1–2 s bayan haɗin har sai tantanin halitta ya yi ƙasa da 80 °CZafin tantanin halitta a lokacin saki, ba saitin lokacin da aka sa ba
Ladubban girke-girkeKololuwa 5–10 °C ƙasa tare da dogon riƙewa, ɗakin karatu ɗaya ga kowane kauri na wafer da ƙayyadaddun ribbonCewa girke-girken da ke kan injin ya dace da samfurin da ke kan bel

1. Rage gangaren gaba-zuwa-baya kafin wani abu

Mafi arha babban ingantawa shine teburin dumama mai ƙarancin zafin jiki a gaban yankin walda, wanda zai kawo fuskar gaba zuwa 80–100 °C domin baya ba dole ba ya yi dukan aikin. Haɗe da wutar da aka raba — yankunan ƙarshe 10–15% ƙasa da tsakiya — tantanin yana isa kololuwa da ƙaramin gangare a cikin kaurinsa. Tsarin matakai uku na dumama, walda da riƙewa ya maye gurbin hawan da saukowar kwatsam da ke kulle damuwa a ciki. Domin yanayin zafin bugun infrared a kan ƙananan tantanoni, bayanan da aka auna na bayanin martaba shine abin da ya dace.

2. Cire tashin hankali daga ƙarshen

Sarrafa tashin hankali mai madauki ba ya kawar da raguwar ribbon, amma yana kiyaye tashin hankali akai-akai daga farkon reel zuwa ƙarshen reel, wanda shine inda yawancin karkacewa ke shiga. Rage sassan ƙarshen da 20–30% dangane da tsakiya yana barin ribbon ya ragu ba tare da jan gefen tantanin ba, kuma barin 0.5–1 mm na sassauci a kowane ƙarshen yana ba da wurin da raguwar za ta tafi. Idan ribbon ya zo da nasa saura damuwa daga zane, annel mai ƙananan zafin jiki kafin ya hau injin yana kawar da wani abu mai canzawa da ba za ka iya sarrafawa ba.

3. Rarraba tantanin kafin su isa injin walda

Ma'aunin karkacewa a mai ɗauka da kwano biyu ko uku sun isa. Ƙwayoyin tantanin da ke da matsanancin damuwa suna gudanar da wani girke-girke daban, mai laushi maimakon ja dukan layin zuwa matsayinsu na yau da kullum, kuma tashar annel ta farko a 100–120 °C na kusan 30 s tana sakin wani ɓangare na damuwar da ke shigowa yayin da tantanin har yanzu yake kwance kuma ba a tallafa masa ba. Wannan shine hanyar da ta fi ƙarancin kuɗi kuma ana tsallake ta mafi yawa, saboda tana gaban injin maimakon cikinsa.

4. Riƙe dukan tantanin, ba tsakiya ba

Cikakken dandali mai faɗi mai ramuka tare da vacuum a gefuna yana cire hinge ɗin. Cikakken bayani da ke yanke shawarar ko zai yi aiki shine sakin: riƙe na 1–2 s bayan haɗin, har sai tantanin ya yi ƙasa da 80 °C, yana barin tantanin ya yi sanyi a ƙarƙashin takura maimakon ya tashi da zarar bututun ya ɗaga. Yawancin layukan da ke girka vacuum na gefe kuma ba su ga wani canji suna sakawa da wuri, kuma gyaran yana buƙatar na'urar ƙidayar lokaci maimakon inji.

5. Rage kololuwa a hankali maimakon bin ta

Kololuwa mai ƙasa da 5–10 °C tare da riƙe mai tsawo yana samar da haɗin da yake da ƙarfi ɗaya tare da ƙarancin damuwa da aka kulle — muddin solder ɗin yana gudana da gaske. Wannan yanayin shine dalilin da ya sa ɗakunan ajiyar girke-girke suke da muhimmanci: kaurin wafer da ƙayyadaddun ribbon duk suna canza taga, kuma layin da ke gudanar da samfura uku akan ɗakin ajiya ɗaya yana inganta don matsakaicin hanyoyi uku daban-daban. Riƙe ɗakin ajiya ɗaya ga kowane haɗi kuma sa injin ya zaɓe shi, ba ma'aikaci ba.

Zane mai panel biyar na hanyoyin sarrafa karkacewa tare da saitunan manufarsu

Hanyoyin biyar ɗin ba madadin juna ba ne. Kowanne yana cire wani kaso na rashin daidaito ɗaya.

Abin da irin wannan canji yake bayarwa a zahiri

Layin samarwa mai yawa na tuntuɓar baya wanda ya yi amfani da hanyoyin guda biyar tare ya ba da rahoton cewa matsakaicin karkacewar bayan ɗaurin igiya ya ragu daga 1.2 mm zuwa ƙasa da 0.5 mm, tare da raguwar ƙin yarda da ke da alaƙa da karkacewa da fiye da 85%. Lambobin da ke ƙasa sun bi shi: matsakaicin wurin ajiye kayan da aka yi watsi da shi da kuma adadin fashe-fashen ƙananan a lokacin lamination duk sun ragu, wanda shine ɓangaren da ke da mahimmanci a kasuwanci saboda ana lissafa su akan tashoshin ajiye kaya da lamination maimakon na ɗaurin igiya.

Ka ɗauki wannan a matsayin sakamakon da aka ruwaito daga layi ɗaya, ba tabbaci ba. Abin da ke canjawa shine hanyar: auna karkacewa a wani tazara da aka bayyana akan samfurin guda ɗaya kafin da bayan, riƙe duk sauran abubuwa a daidai, sannan ka canza hanyoyin a tsarin da ke sama. Layin da ke canza abubuwa biyar a lokaci ɗaya kuma ya sami ingantaccen lamba ba ya koyon wani abu da zai iya maimaitawa a kwata na gaba.

Tabbacin da ke shawo kan abokin ciniki ba lambar karkacewa ce kawai ba. Ita ce nau'i biyu na hotuna masu dacewa — EL bayan ɗaurin igiya da EL bayan lamination akan igiya ɗaya — tare da rarraba wurin ajiye kayan a duk tsawon aiki. Karkacewa wakili ne kawai; abubuwan biyu da kake damuwa da su da gaske sune haɗin gwiwa da ke tsayawa cikakke da gefen pad ɗin da robot ɗin zai iya samu har yanzu bayan an danna module ɗin ya zama lebur.

Muna kwatanta hotunan electroluminescence kafin da bayan matakin lamination a kowane gwajin, muna duba ko igiyoyin da ke da karkace har zuwa 1.2 mm suna samun microcracks lokacin da aka matse su a kwance cikin zafi.

Tarko uku da ke sa layi ya tsaya

Rage zafin jiki ba tare da wani abu ba. Rage kololuwar zafi yana rage wani abu a cikin rashin daidaituwa kuma yana ƙara haɗari nasa: ƙila Layer intermetallic ba ta samu yadda ya kamata ba kuma haɗin ya zama haɗin sanyi wanda ke wucewa duba gani. Zafin jiki shine hanya mafi sauƙi da za a kai kuma mafi ƙarancin tasiri shi kaɗai.

Sake amfani da girke-girken tuntuɓar gaba. Tantanin tuntuɓar baya ya bambanta a fuskar da ake walda, kaurin wafer da sashin ribbon. Girke-girke shine jerin lambobi da suka dace da haɗin ɗaya daga cikin waɗannan uku, kuma sake amfani da shi ba gajeriyar hanya ba ce illa tsarin da ba a gwada ba da ke gudana a samarwa.

Daidaita na'urar walda yayin watsi da damuwa mai shigowa. Tare da fiye da 30% na gudummawar da ke zuwa kafin tantanin ya isa injin, layi na iya shafe makonni a yankin walda kuma ba zai taɓa kaiwa manufa ba. Rarrabewa da pre-annealing a wurin lodi ba abu ne mai ban sha'awa ba kuma shine inda sauran rata yawanci yake.

Tambayoyin da ake yawan yi

Shin ƙarshen warp ya keɓanta da ƙwayoyin da ke da alaƙa da baya?

Tsarin ba haka ba ne, amma tsananin haka ne. Ƙwayoyin da ke da alaƙa da gaba suna nuna irin wannan rashin daidaituwar zafi kuma suna shanye shi saboda ƙarfen gaba yana yada zafi kuma wafer ɗin ya fi kauri. Ƙwayoyin da ke da alaƙa da baya suna haɗa dumama gefe ɗaya, siraran wafer da siririn ribbon, wanda shine dalilin da ya sa stringer ɗaya ke samar da warp mai karɓuwa akan samfur ɗaya da siffar jirgi akan ɗayan.

Wane adadi na warp ne layin ya kamata ya nema?

Ƙasa da haƙurin sanya wurin ajiye, tare da rata. Idan ajiye yana buƙatar ±0.5 mm, manufa ta 0.5 mm ba ta barin komai don bambancin rukuni. Layukan da ke ba da rahoton nasara suna ƙasa da 0.5 mm a matsakaici tare da ƙarshen da aka tsare, wanda shine dalilin da ya sa adadin ƙin yarda yake da muhimmanci kamar matsakaici.

Za a iya gyara stringer da vacuum na gefe?

Yawanci i, akan injuna waɗanda platen ɗinsu module ne mai maye gurbin maimakon wani ɓangare na firam ɗin. Nemi zanen platen da taswirar yankin vacuum kafin ɗauka cewa abin hawa ne kawai; akan wasu dandamali canjin yana shafar rarraba vacuum da jerin saki, ba kawai farantin ba.

Shin ƙananan zafin kololuwa yana rage yawan kayan aiki?

Yana rage yawan shigar da zafi, don haka yawanci dole ne lokacin jira ya tashi don kiyaye haɗin gwiwa lafiya. Ko hakan yana rage yawan kayan aiki ya dogara da ko injin ɗin yana da iyaka ta lokacin jira ko ta index. Stringer da ke gudana ƙasa da ƙayyadadden zagayowar sa yawanci yana da iyaka ta index, kuma dogon lokacin jira ba ya kashe komai; duba wace ƙuntatawa kake ciki kafin musayar lokacin zagayowar.

Me ya sa warp wani lokaci yakan zama mafi muni bayan kwana ɗaya?

Damuwa da ta rage tana ci gaba da sassautuwa bayan string ɗin ya huce. Awo da aka yi a mashigar injin yana ɗaukar ɓangaren elastic; ɓangaren viscoelastic yana tasowa cikin sa'o'i. Auna a sa'o'i 0, 1 da 24 a kan samfurin idan korafe-korafen da ke ƙasa ba su dace da lambobin da kake rubutawa a stringer ba.

Shin haɗin 0BB yana canza hoton warp?

Suna canza lokaci. Haɗin manne da na fim suna motsa wani ɓangare na haɗin zuwa laminator, don haka ƙarancin zafi yake shiga cikin tantanin a stringer kuma ƙarancin damuwa yake kullewa da wuri. Ciniki shi ne cewa lahani suna bayyana daga baya, bayan lamination, lokacin da module ɗin ya fi daraja. Dabarun riƙewa da sanyaya har yanzu suna aiki; wurin awo yana motsawa.

Shin warp dalili ne na ƙin mai samar da tantanin?

Kawai da bayanai. Warp mai shigowa yakan bambanta da kowane rukuni, kuma mai kaya da ya yi kama da mara kyau a rukuni ɗaya na iya zama matsakaici a cikin goma. Rarraba da girke-girke na musamman yawanci suna dawo da amfanin ba tare da canza masu kaya ba; canjin ƙayyadaddun bayanai shine matakin da ya dace lokacin da rarraba kanta ta canza kuma ta ci gaba da canzawa.

Wanne daga cikin masu amfani biyar ne sabon layi ya kamata ya fara ƙayyade?

Riƙon cikakken faɗi da wutar yankin ƙarshen da aka raba, saboda waɗannan ana yanke shawara lokacin da aka ƙayyade injin kuma suna da tsada a ƙara daga baya. Preheat da sarrafa tashin hankali yawanci ana samun su azaman zaɓuɓɓuka; rarraba mai shigowa da pre-anneal shawarwari ne na tsari da za ka iya yankewa a ranar farko ba tare da siyan komai ba.

Kwatanta kafin da bayan warp bayan stringing da adadin ƙin da ke da alaƙa da warp a layin samar da yawa na back-contact

Layi ɗaya da aka ruwaito, masu amfani biyar tare. Hanyar tana canjawa; lambar mafari ce, ba alkawari ba.

Tunani na ƙarshe

Ƙarshen warp shine alamar bayyane ta tsarin gefe ɗaya da ke gudana akan ƙaramin tantanin halitta da aka riƙe a wurin da bai dace ba. Gyara shi ba batun neman madaidaicin zafin jiki ɗaya ba ne; saituna biyar ne waɗanda kowanne yana cire wani kaso na rashin daidaito ɗaya, kuma waɗanda suka fi amfani yawanci su ne waɗanda suke wajen yankin walda — tantanin da aka jera, an riga an yi masa annealing da kuma platen da ke riƙe faɗin gabaɗaya har sai haɗin ya yi sanyi.

Idan kana ƙayyade dandamali don samar da back-contact, tambayar da za a yi ba ita ce wace kololuwar zafin jiki yake kaiwa ba amma yadda yake riƙewa da sakin tantanin 110 µm. Amsar ita ce za ta yanke shawarar yawan amfanin da za ka bayar a wata na shida.

Ga modules na back-contact masu saurin kamuwa da lanƙwasawar tantanin halitta da damuwar haɗin gwiwa, OOITech na gina ɗaki ɗaya da biyu injin laminator na panel na hasken rana tare da platens masu dumama mai ko na lantarki don sarrafa daidaiton zafin jiki. Aiko mana da zanenka, tarin module, ko samfuran igiya don kimanta tsari, kuma za mu tabbatar da sigogin girke-girke akan kayan gwajin mu.


Tags :

Nemi Farashi

Duk abubuwan da aka ɗora suna da tsaro kuma sirri ne.

Me ya sa Zaɓe Mu

Muna isar da gwanintar da za ka iya amincewa sabis ɗinmu

Kayan aiki kai tsaye daga masana'anta.

Fa'idodin Rage Kuɗi

Muna ba da ƙima ta musamman, muna haɓaka sakamako yayin da muke rage kasafin kuɗi ga abokan ciniki.

Ƙungiyar Ƙwarewarmu

Kwararrun ma'aikatanmu sun ƙware a sababbin hanyoyin magance matsaloli da dabarun da aka keɓance.

Fiye da Shekaru 15 na Ƙwarewar Masana'antu

Ƙwarewa mai zurfi tana tabbatar da sakamako masu dogaro, masu bin zamani, da tabbatattu don nasara.

Shaidun Abokan Ciniki

Abin da Abokin Cinikinmu Ya ce game da mu

Shaidun abokan ciniki sun yaba da zurfin fahimtarmu game da ƙalubalen su, wanda ke haifar da sababbin hanyoyin magance matsaloli da riba mai ƙarfi. Haɗin gwiwa na dogon lokaci—wasu fiye da shekaru goma—suna nuna amincewarsu da gamsuwa. Labaran nasarar su suna motsa mu don ci gaba da wuce tsammanin su. Ƙara Sani

Kayayyakin Mu

Sabbin Kayayyakin Mu

PV Backsheet don Solar Modules — TPT, KPK, PVDF
2025-09-09 17:03:06

PV Backsheet don Solar Modules — TPT, KPK, PVDF

PV backsheet don solar modules a cikin TPT, KPK, PVDF da kuma bayyanannun nau'ikan: mai jure UV, mai hana wutar lantarki da kuma kariya ta baya mai hana danshi.

Kara Karantawa
OTCT Mai Gwajin Kwayar Rana: IEC 60904-9 A Grade
2025-09-08 13:53:04

OTCT Mai Gwajin Kwayar Rana: IEC 60904-9 A Grade

OTCT-A gwajin tantanin hasken rana – fitilar xenon mai darajar A, 16-bit 4-ch samu, IEC60904-9:2020. Ingantaccen ma'aunin lanƙwan IV don mono &

Kara Karantawa
CHT9951A Mai Gwajin Hipot: Rufe Rukunin PV 0.1-10kV
2025-09-08 14:34:35

CHT9951A Mai Gwajin Hipot: Rufe Rukunin PV 0.1-10kV

CHT9951A/CHT9951B na'urar gwajin hipot da juriya ta insulation don gwajin PV module na hasken rana. Fitarwar DC har zuwa 10kV, juriya ta insulation har zuwa 99GΩ

Kara Karantawa
HDX200-P Injin Bussing na Rabin Sel: Zagayowar 18s
2025-09-05 22:09:45

HDX200-P Injin Bussing na Rabin Sel: Zagayowar 18s

HDX200-P Half Cell Auto Bussing Machine tana da walda ta hanyar electromagnetic induction tare da kawunan walda 18, lokacin zagayowar ƙasa da daƙiƙa 18

Kara Karantawa
Injin Manne da Firam da Manne na J-Box: Tafiyar 2500mm
2025-09-06 13:30:26

Injin Manne da Firam da Manne na J-Box: Tafiyar 2500mm

Ooitech yana bayar da ƙwararrun injunan manne frame na atomati (SPZ-2400GS-T2-Y2) tare da famfon ARO na Amurka da tsarin GRACO PCF

Kara Karantawa
Na'urar firam ɗin panel ɗin hasken rana ta OTZK: ±1mm, 2000x1100mm
2025-09-08 15:04:22

Na'urar firam ɗin panel ɗin hasken rana ta OTZK: ±1mm, 2000x1100mm

Ooitech yana ba da injunan yin fom na faifan rana masu inganci, ciki har da injin fom na buga ruwa da injin fom na atomatik OTZK-A

Kara Karantawa
Gajeriyar hanyar bincike ta AI

Tambayi AI Game da OOITech

Danna ɗaya yana buɗe mataimakin AI ɗinka tare da tambaya game da layukan samar da fale-falen hasken rana da muke ginawa an riga an cika su — layukan PV na turnkey da muke ginawa, daga rabin-atomatik zuwa sikelin GW, da abin da farashi ke buƙata.

Samu Faɗi