Alhakin edita na wannan labarin yana hannun Wuhan Ooi Photoelectric Technology Co., Ltd. An rubuta kuma an duba shi daga ƙungiyar edita ta Ooitech. Duba manufar edita don yadda muke rubutu, inda ake amfani da kayan aikin AI, da yadda za a nemi gyara.
Menene Ake Ƙidaya a Matsayin Module na Solar Mai Sauƙi na Gaske?
Teburin Abubuwan Ciki
Amsa mai sauri: Ƙaramin ƙarfin hasken rana mai sauƙi ana bayyana shi ta hanyar abin da tsarin ɗora zai iya ɗauka, ba ta wani adadi na nauyi da aka zaɓa ba. Kasar Sin tana da babban ajiya na rufin masana'antu da na kasuwanci inda ba a taɓa tsara tsarin don wani na'ura ta gilashi-gilashi ko gilashi-baya ba, don haka nauyin na'urar da za a iya amfani da shi ana kayyade shi ta ragowar iyakar nauyin rufin maimakon ta kas ɗin samfuran. Samun ƙaramin nauyi yana zuwa ne daga rage kaurin gilashi, yin amfani da ƙaramin firam mai sauƙi ko cire firam ɗin gaba ɗaya, da zaɓar takardar baya mai sauƙi. Kauri a cikin aji na 6 mm da 4.75 mm sun bayyana a cikin gine-ginen na'urar da aka tattauna, idan aka kwatanta da gilashin gaba na al'ada na 3.2 mm ko fiye. Kowace raguwa tana musanya ƙimar nauyin inji da juriya ga tasiri, don haka ƙayyadaddun dole ne ya fara daga rufin da zai zauna a kai.
PV Module Manufacturing · na Jerry, Ooitech
Gabatarwar Samfur
China tana da babban tarin wuraren masana'antu da kasuwanci inda rufin ko tsarin ba zai iya ɗaukar nauyi mai yawa ba. Misalin PV module yana kusan 10.6kg a kowace murabba'in mita. Yawancin tsofaffin rufin ƙarfe masu launi da tsarin musamman ba za su iya kaiwa wannan lambar ba, don haka ba za ku iya sanya daidaitattun bangarori a kansu ba.
Wannan shine inda ƙananan nauyin modules suka shigo. Abubuwan amfani suna da yawa: rufin masana'anta na ƙarfe mai launi, PV na facade na gini, sassauƙan hawa a kan tafkunan ruwa da tashoshin kula da najasa, rufin da ba a iya tafiya, carport canopies, PV curtain walls, da ƙari. Wasu ƙididdiga sun nuna cewa buƙatar cikin gida na ƙananan nauyin modules ya kai dubun gigawatts.
Dubi yadda wannan ya kasance. Masu fara wasa na farko waɗanda suka yi fare musamman akan nau'ikan hasken rana masu sassauƙa, kamar Ritek da SunMan, duk sun ɓace. Yawancin ayyukansu na farko sun nuna matsalolin aminci. Nau'ikan hasken rana masu sassauƙa suna da raunin bayyananne a waɗannan yanayi, amma buƙatar kasuwa har yanzu tana nan. A kan wannan yanayin, Zhongnengchuang ya ƙaddamar da "nau'in hasken rana mai ƙarfi-sassauƙa" kuma ya zama jagora a wannan fanni.
Me yasa Nau'ikan Hasken Rana Masu Sassauƙa Ke Kasawa a Waɗannan Yanayi
Ƙananan lahani guda biyu na nau'ikan hasken rana masu sassauƙa da aka liƙa
Nau'ikan hasken rana masu sassauƙa na gargajiya suna barin gaban gilashin da aka ƙarfafa kuma galibi suna dogara da mannewa don liƙa duka panel ɗin a kwance a saman ƙasa. Wannan shigar da aka liƙa gabaɗaya yana da lahani biyu masu mutuwa.
Na farko, panel ɗin yana zaune kusa da ƙasa ba tare da tazarar iska ba. Rashin zafi yana da muni, yanayin aiki yana tashi sosai, kuma raguwar ƙarfin lantarki yana sauri.
Na biyu, da zarar wuri mai zafi ya bayyana a cikin wannan tsarin da aka liƙa, zafi ba shi da inda zai tafi, don haka haɗarin wuta yana ƙaruwa sosai. Bugu da ƙari, ba tare da kariyar gilashin da aka ƙarfafa ba, juriya ga ƙanƙara da tsufa na UV yana da rauni. Idan aka yi amfani da shi a waje na dogon lokaci, yana iya yin kumfa da rabuwa, don haka haɗarin kulawa yana da yawa.

Ma'aunin Fasaha
Tsarin ƙarfi-haske vs tsarin haske na al'ada
Ɗauki misalin tsarin haske na LONGi's Hi-MO X10. Dukansu suna cikin nau'in haske, amma hanyoyin fasaha na asali sun bambanta sosai.
| Abu | LONGi Hi-MO X10 Haske | Zhongnengchuang Ƙarfi-Haske |
|---|---|---|
| Hanyar ƙira | Inganta ƙaramin firam na aluminum | Babu firam na aluminum, gefen cikakken rufi na siriri |
| Firam | Firam na aluminum alloy mai anodized | An cire |
| Gilashi | Gilashi mai rabin ƙarfi na 1.6mm | Gefen cikakken rufi na siriri |
| Nauyi | 16.3 ± 3.3 kg | Ƙananan nauyin fili |
| Girma | 1990 x 1134 x 30 mm | Jimlar kauri kawai 4.75 mm |
| Nauyin fili | Kimanin 7.2 kg/m² | Ƙarƙashin 5.91 kg/m² |
| Saka | Yawanci manne da clamps, bai dace da manna babban yanki ba | Ƙugiyoyin baya + rack, ko manna a kan ƙarfe mai launi / ƙarfe mai murabba'i |
Sigar LONGi ta dogara da aluminum profile don kariyar injiniya. Fasahar ta balaga kuma tana shigar da yawanci tare da clamps, wanda bai dace da manna babban yanki ba.
Rigid-light module na Zhongnengchuang ya watsar da nauyi aluminum frame kuma yana amfani da 4.75mm ultra-thin composite full-wrap edge. Jimlar kauri shine 4.75mm kuma nauyin areal ya ragu zuwa 5.91kg/m², kusan 18% fiye da lightweight module na LONGi. Saka na iya zama ƙugiyoyin baya + rack, ko manna a kan ƙarfe mai launi ko ƙarfe mai murabba'i.

Rigid-light module na Zhongnengchuang VS na al'ada lightweight module

Fa'idodin Fasaha
Ƙananan nauyin fili: zuwa 5.91 kg/m², ƙasa da 10.6 kg/m² na daidaitattun modules kuma kusan 18% fiye da lightweight aluminum-frame module
Ultra-thin gini: jimlar kauri kawai 4.75mm tare da composite full-wrap edge maimakon nauyi aluminum frame
Saka mai sassauƙa: yana aiki da ƙugiya na baya tare da raki, ko manna kai tsaye akan karfe mai launi ko karfe mai murabba'i
Ingantacciyar aminci fiye da mai sassauƙa: yana kiyaye kariya mai ƙarfi don haka yana guje wa kumfa, ɓarna da haɗarin zafi da ke addabar fale-falen da aka manna gaba ɗaya
Ya dace da yanayin rauni mai rauni: ya dace da wuraren da ba za a iya shimfiɗa daidaitattun kayayyaki ba
Aikace-aikacen Samfur
Wannan nau'in na'urar mai sauƙi yana kaiwa ga manyan wuraren da ke da iyakacin ƙarfin ɗaukar nauyi. Abubuwan amfani na yau da kullun sun haɗa da rufin masana'anta na karfe mai launi, PV na bangon gini, shimfiɗa mai sassauƙa akan tafkunan ruwa da tashoshin kula da najasa, rufin lanƙwasa, rufin da ba a iya tafiya, rufin mota, da bangon PV.
Jagorar shigarwa



















Ra'ayin Ooitech
Gaskiyar abin da za a fahimta a nan ita ce nauyi kadai bai taba zama cikakken labari ba. Tsarar da ke da sassauci mai tsafta ta rasa kasuwa saboda sun bar kariya mai tsauri da iskar da ke kiyaye tsarin rayuwa a waje sama da shekaru 20. Gefen nannade na 4.75mm wanda har yanzu yana ba ka damar manna a kan karfen launi ko rataya a kan raki hanya ce mai wayo ta tsakiya. Daga bangaren masana'anta muna ganin wannan yanayin a kan layukan samar da mu, gilashin sirara da ƙirar marasa firam suna buƙatar ƙarin tsauraran lamination da sarrafa firam, don haka kwanciyar hankali na tsari yana da muhimmanci kamar lissafin kayan aiki. Idan kana son ganin yadda waɗannan layukan masu nauyi da marasa firam ke aiki a ƙasa, tashar Ooitech YouTube a www.youtube.com/ooitech yana da daraja a bi.
Ƙarin karatu da bayanan baya
Kayan tunani na jama'a kan wannan batu, wanda ƙungiyoyin da ke kula da taswirar fasahar masana'antar da bayanan kasuwa suka wallafa: