Alhakin edita na wannan labarin yana hannun Wuhan Ooi Photoelectric Technology Co., Ltd. An rubuta kuma an duba shi daga ƙungiyar edita ta Ooitech. Duba manufar edita don yadda muke rubutu, inda ake amfani da kayan aikin AI, da yadda za a nemi gyara.
LONGi ACM: Abin da Metallization Mara Azurfa Ke Yi ga Haɗin Gwiwa
Teburin Abubuwan Ciki
Amsa mai sauri: ACM ita ce ƙarfe mara azurfa ta LONGi don tantanin halitta mai tuntuɓar baya, wanda aka sanar a watan Yuli 2026 kuma ana samar da shi da yawa a cibiyarsa ta Xixian. Yana tara abubuwa uku: Layer na iri da shamaki wanda ke hana tagulla shiga cikin silicon, mai gudanar da tagulla da aka buga da kayan aikin allo da ake da su, da kuma tsarin tuntuɓar matrix wanda kowane abin lantarki ke da babban ɓangaren jigilarwa da ƙaramin wurin tuntuɓa. Adadin da aka wallafa sune ingancin tantanin halitta na 27.6% wanda ISFH ta tabbatar, 672 W wanda TUV Rheinland ta tabbatar, 0.2 zuwa 0.3 maki na ribar tantanin halitta, 3 zuwa 5 W na ribar module, da kusan 80% ƙarancin haɗarin karyewar yatsa. Abin da ke isa ga igiyar jeri ya fi wannan guntu: sandar lebur da za a haɗa, ƙarfe wanda ya riga ya cinye matakinsa na ƙarshe na zafin jiki mai girma, hanyar tuntuɓa da ke gudana ta wurare daban-daban, kuma babu bayanan fili har yanzu.
Abin sha'awa na ACM ba rashin azurfar ba ne. Shi ne cewa an sake fasalin abin lantarki zuwa sassa biyu, kuma ɗaya kawai daga cikinsu shine saman da ribbon ɗinka ke sauka a kai.
Abin da LONGi ya ƙaddamar, da kuma lokacin
LONGi ya sanar da ACM a watan Yuli 2026 a matsayin nano-alloy matrix contact kuma ya ce ya kai ga samar da yawa a Xixian. Kamfanin yana gabatar da shi a matsayin ainihin silver-free metallization don layin sa na baya, wanda ya dace da HPBC, HIBC da BC 2.0. A tsarin LONGi, wani yanki ne na babban tsari: conductive backsheet yana kula da gine-gine, shingling da hidden busbars suna kula da tsari, ACM kuma yana kula da ƙarfe.
Wata magana ta taka tsantsan ya kamata ta kasance kusa da saman. LONGi bai wallafa abun da ke cikin alloy ko ragowar abun da ke cikin silver ba, kuma wani bita na baya kan hanyoyin da ba su da silver a wannan shafin ya riga ya sanya ACM cikin rukunin paste na copper maimakon cikin rukunin copper tsantsa. Karanta jimlar game da maye gurbin silver paste a matsayin bayanin wani abu, ba gwaji ba.
Lissafin silver, da kuma dalilin da ya sa ƙarfe ɗaya bai isa ba
Ajiyar silver da aka tabbatar kusan tan 640,000 ne, yawan haƙoƙin shekara kusan tan 32,000, kuma masana'antar photovoltaic ta riga ta ɗauki fiye da kashi ɗaya cikin huɗu na amfani da duniya. Majiyar ta ƙara wani hasashe da ake maimaitawa sosai: idan an samar da 1,000 GW a shekara na samar da module, masana'antar za ta ƙare da silver mai araha cikin shekaru goma.
Ana faɗin wannan lambar sau da yawa fiye da yadda ake tantance ta. Kashi ɗaya cikin huɗu na tan 32,000 shine tan 8,000 a shekara, kuma 640,000 da aka raba da 8,000 yana bada shekaru 80, ba 10 ba. Sigar shekaru goma tana aiki ne kawai idan buƙatar PV ta ƙaru sau da yawa daga nan, don haka yanayin haɓaka ne, ba lissafin ajiya ba. Adadin da ke da mahimmanci a kasuwanci ya fi ƙanƙanta: tan 8,000 a kan GW 1,000 shine mg 8 a kowace watt, don haka module na 672 W yana ɗauke da kusan g 5.4 na azurfa.
Tsohon amsar ga farashin azurfa ita ce joometry. Yatsu na gaba sun tashi daga kusan micrometers 110 zuwa ƙasa da 20 a yau, kuma kowane micrometer da aka cire yana ɗauke da ɓangaren giciye na gudanarwa. Yatsu masu sirara suna ƙara juriya, kuma a ƙarshe suna karyewa, ɗagawa ko kasa jika. Wannan shine triangle da tushen ya bayyana, tare da azurfa a tsakiya.
Copper yana gudanarwa kusan kamar azurfa kuma farashinsa ya fi ƙasa da yawa, don haka me zai hana a sauya paste ɗin kawai? Abubuwa biyu ne suka amsa. Copper oxide ya fi kusa da insulator fiye da conductor, don haka yatsan da ya yi oxidized yana daina aiki maimakon tsufa a hankali. Kuma copper yana yaduwa cikin silicon da sauri fiye da azurfa, yana haifar da matakan zurfi waɗanda ke rage rayuwa kuma, a wurin tuntuɓar, hanyar da current bai kamata ya gudana ba. Li Zhenguo ya rufe shi a layi ɗaya: a ƙarshe, ba mu zaɓi ƙarfe ɗaya ba.
Yadudduka uku, aiki ɗaya kowanne
Na farko shine iri da fim ɗin shinge mai kauri na 'yan nanometers tsakanin silicon da madugu. Yana yin abubuwa biyu: yin haɗin ohmic mai ƙarancin juriya da silicon ɗin da aka yi wa doping, da hana jan ƙarfe shiga cikinsa. Majiyar ta ce masana'antar suna hasashe game da nickel, wanda zai samar da nickel silicide, ko shingen titanium tungsten. LONGi bai tabbatar da ɗaya ba.
Na biyu shine madugu, wanda aka bayyana a matsayin manna gami da ƙarfe da yawa maimakon sinadari ɗaya, an lulluɓe shi da harsashin polymer wanda ke hana iskar oxygen shiga cikin ƙarfen da ke ƙarƙashinsa. Da'awar da ke tattare da shi ita ce dacewa da bugu na allo, wanda shine dalilin da ya sa labarin gyaran ya kasance gajere: injin bugu ɗaya, manna daban.
Na uku ba Layer ba ne kwata-kwata amma tsarin siffa ne, kuma shine ɓangaren da ke canza abin da injin stringer ke gani.
| Mataki | Menene shi | Abin da yake yankewa a haɗin gwiwa |
|---|---|---|
| Iri da shinge | Fim mai sikelin nanometer tsakanin silicon da madugu; majiyar ta ce masana'antar suna hasashe game da nickel ko shingen titanium tungsten | Juriya ta haɗuwa, da yawan zafi da mahaɗin ke ɗauka kafin shingen ya daina zama shinge |
| Madugun gami da jan ƙarfe | Wani manna na gami da ƙarfe da yawa da aka buga da kayan aikin allo, an naɗe shi a cikin harsashi na polymer wanda ke hana iskar oxygen shiga cikin ƙarfen | Kaurin ƙarfen da ribbon ɗin ke zaune a kai, da zafin saman da yake jurewa ba tare da rasa harsashinsa ba |
| Tuntuɓar matrix | Tsarin maki inda wutar lantarki ke shiga cikin silicon, tare da wani ɓangaren jigilar da ya fi faɗi a sama wanda ke fitar da ita | Nawa yanki ribbon ɗin ke haɗawa da shi, da yadda ake auna ƙarfin ja da zagayowar zafi |
Hanyar rigar da yake maye gurbinsa
Plating ita ce hanyar da masana'antar ke amfani da ita shekaru da yawa. Matakanta:
- Sanya Layer na shamaki da Layer na iri a saman tantanin.
- Rufe dukan saman da abin rufewa, sannan a fallasa shi a haɓaka tsarin.
- Cire iri da shamaki a duk inda aka cire abin rufewar.
- Cire sauran abin rufewar da laser, sannan a tsaftace oxide daga iri da acid.
- Sanya jan ƙarfe a cikin buɗaɗɗen wuraren don gina lantarki.
Kowane ɗayan waɗannan matakan jika ne ko lithographic kuma an yi rajista zuwa na ƙarshe. Da'awar ACM ita ce gami da aka buga ya maye gurbin jerin, wanda shine dalilin da ya sa LONGi ke kiran gyaran da sauƙi: babu benci na plating, babu abin rufe fuska, babu tsiri. Majiyar tana kiran sakamakon da busasshiyar, sauƙaƙan sigar plating.
Lambar da za a riƙe ita ce rabon aspect. Sau biyar zuwa bakwai na yanki a faɗin da ya fi ƙunci ba ƙaramin matsalar rheology ba ne, kuma idan ya riƙe a girma ya cancanci dubawa akan sel masu shigowa maimakon kan slide. Yanke mai gogewa da bincike mai maki huɗu ba sa buƙatar bayyanawa daga mai kaya.
Electrode ɗin yana da sassa biyu, kuma ɗaya ne kawai daga cikinsu haɗin gwiwa

Electrode ɗaya, ayyuka biyu. Ribbon ɗin yana haɗawa da sandar jigilarwa; wurin tuntuɓar da ke ƙasa yana saita sake haɗuwa, kuma zafin haɗawa yana gudana kai tsaye zuwa gare shi. Tsarin kamar yadda aka bayyana a cikin kayan ƙaddamar da LONGi, an sake zana shi cikin Turanci.
A cikin electrode ɗaya akwai siffofi biyu. Wani ɓangaren tuntuɓa yana wucewa ta buɗe wani abu a cikin passivation kuma yana taɓa Layer ɗin da aka yi doping a kan ƙaramin yanki. Wani ɓangaren jigilarwa shi ne faffadan sandar lebur da ke sama da shi, yana ɗaukar wutar lantarki a gefe zuwa ribbon ɗin. Hoton yana nuna duka ra'ayoyin.
Dalilin lissafi ne. Asarar haɗuwa tana ƙaruwa da yanayin saduwa kuma asarar juriya tana ƙaruwa da yanki, don haka ƙirar ta raba su. Kwatancen Li a cikin tushen jirgin ƙasa ne mai sauri wanda ke tsayawa a tashoshi kawai: wutar lantarki tana shiga a wurare kaɗan sannan ta yi tafiya mai nisa ba tare da biyan kuɗi ba.
Ga layin module ɗaya sakamako ɗaya yana da sauƙin mantawa. Ribbon ɗin ba ya haɗuwa da wurin saduwa amma ga sandar jigilar, wadda take lebur, mai faɗi kuma an buga ta maimakon ƙone ta, yayin da duk abin da ke ƙarƙashin zafi yake a wuri. **Haɗin ba ya taɓa silicon. Yana taɓa sandar da ke ciyar da wuraren, kuma zafinsa yana gangarowa kai tsaye zuwa mafi ƙanƙantar sashi na shingen.**
Don haka ƙarfin ja yana na kowane pad, domin yankin haɗin shine sandar kuma sandar ba tantanin ba ce. Haƙurin sanyawa yana na gefen pad. Kasafin zafi yana na tarin tantanin, wanda ba shi da matakin ƙonewa don ɗaukar wuce gona da iri.
Abin da LONGi ta wallafa
Lambobin da ke ƙasa kamar yadda LONGi ta wallafa kuma aka ruwaito a cikin tushen, tare da sunan hukumar tabbatarwa inda aka ambaci ɗaya. Babu wanda muka auna.
| Ma'auni | Hoto | Matsayi |
|---|---|---|
| Ingancin tantanin, bayanan girma | +0.2 zuwa 0.3 maki | LONGi, kamar yadda aka ruwaito |
| Ƙarfin module, bayanan girma | +3 zuwa 5 W | LONGi, kamar yadda aka ruwaito |
| Ingancin tantanin halitta, tabbatacce | 27.6% | ISFH, bisa ga tushen |
| Ƙarfin module, tabbatacce | 672 W | TUV Rheinland, bisa ga tushen |
| Yankin yatsa | Sau 5 zuwa 7 na yatsa na al'ada | LONGi, kamar yadda aka ruwaito |
| Juriya ta yatsa | 1/5 zuwa 1/7 na yatsan azurfa | LONGi, kamar yadda aka ruwaito |
| Haɗarin karyewar yatsa | kusan 80% ƙasa | LONGi, kamar yadda aka ruwaito |
| Garanti | 1% shekara ta farko, 0.33% a shekara, shekaru 30 | Sharuɗɗan garanti na LONGi |
Sau biyu na juyawa namu ne. Riba ta 0.2 zuwa 0.3 maki akan tantanin halitta sama da 27% kusan 1% ne na dangi, kuma 3 zuwa 5 W akan module na 640 zuwa 672 W shine 0.5% zuwa 0.8%. Sau biyar zuwa bakwai na yankin a faɗin da ya fi ƙunci yana nufin sau biyar zuwa bakwai na tsayi, wanda shine rabon da bugu dole ya riƙe a samarwa.
Fayil ɗin amincin, da layin da bai ketare ba
Abin da gwaje-gwajen suka nuna
Aikin dakin gwaje-gwaje ya wuce tsarin da aka saba: awanni 2,000 na zafi mai danshi, sau uku jerin zagayowar zafi, da ninki biyu na adadin UV60. Gudanar da zagayowar guda ɗaya ta haifar da sakamakon da ba a shirya ba wanda ya fi wanda aka shirya muhimmanci: fitowar ɗakin ta haura zuwa 150 Celsius, kuma na'urorin ACM sun jure shi yayin da na'urorin al'ada suka nuna ƙananan tsagewa da duhu. Man fatin azurfa ana toya shi da zafi kuma yana riƙe da ramukan da ke shan danshi cikin shekaru; madugu na ACM fim ne na zafin jiki mai ƙasa kuma yana farawa ba tare da shi ba. Sharuɗɗan garanti sun biyo baya: 1% a shekara ta farko, 0.33% a shekara bayan haka, shekaru 30.
A cikin gwaje-gwajen muhalli namu, muna gwada na'urorin da aka lissafta da awanni 2,000 na zafi mai danshi don tabbatar da cewa rufewar tana kiyaye ingancin haɗin kewaye da gami da polymer ke karewa ba tare da rabuwar gefe ko shigar danshi ba.
Abin da ba za su iya nunawa ba
Abin da fayil ɗin ba zai iya rufewa shi ne lokaci. An fara samar da juzu'i a tsakiyar 2026, don haka akwai watanni na fallasa a waje kuma babu wani abu kusa da da'awar shekaru 25. Yanayin gazawar yana jinkiri: jan ƙarfe yana yaduwa ta cikin silicon fiye da sau dubu fiye da azurfa, kuma da zarar ya isa mai fitarwa yana samar da cibiyoyin haɗuwa waɗanda ba sa warkewa. Masana'antar ta gudanar da wannan gwaji: farkon lulluɓe da jan ƙarfe ya wuce gwajin dakin gwaji, sannan ya rasa kayan fitarwa bayan kusan shekaru biyu a fagen. Tsarin LONGi mai yadudduka uku an yi shi ne daidai da wannan tarihin, amma babu wani kamfani da zai iya nuna shekaru 25 na hakan. Lalacewar da yuwuwar haifarwa ita ce misali mai gargaɗi: ta wuce gwaje-gwajen gaggawa, an aika ta, sannan ta bayyana daga baya a fagen.
Madogarar ta sanya kwanan wata a kan gibin. Modulolin da aka rage azurfa da aka yi kafin 2026 suna buƙatar har kusan 2031 don tara shekaru biyar na bayanan waje, kuma a lokacin ne tambayar za ta daina zama muhawara ta zama awo.
Abin da wannan ke canzawa a injin ɗinka igiya
An buga saman, ba a ƙone shi ba. Kushin azurfa fim ne da aka yi sintered, mara aiki sosai; sandar gami a ƙarƙashin harsashi na polymer ba haka ba ce, kuma wannan harsashin shi ne ke wakiltar kwanciyar hankalin azurfa. Duk wani matakin haɗawa da zai ƙone, ya lalata ko ya cire shi da sinadarai yana aiki ne da tsarin.
Kasafin zafi yanzu na tantanin halitta ne. ACM yana cire matakin sintering na zafin jiki mai girma, don haka metallization yana zuwa ba tare da wani tazara na zafi da ya rage ba. Inda rufin yake ya dogara da tarin passivation, kuma tare da Layer na silicon amorphous yana zama ƙasa da bayanin martaba na harbi na al'ada. Tsarin tantanin halitta mai tuntuɓar baya yana saita wannan lissafin; rufin ana saita shi ta duk abin da ke samansa.
Don mutunta ƙananan rufin zafi na waɗannan tarin tantanin halitta, muna gudanar da zagayowar lamination ƙasa da 150 Celsius, ta amfani da yankunan dumama platen daidai don guje wa wuce gona da iri na zafi a kan tuntuɓar da aka buga.
Yankin mashaya ne kuma hanyar aya ce. Yankin haɗi yana bin mashaya jigilar kaya, don haka ribbon mai lebur har yanzu yana da ainihin yanki da zai sauka, yayin da hanyar zafi da ke ƙasa tana gudana ta wurare daban-daban, inda gwajin ja da zagayowar zafi duk suna mai da hankali.
Wace inji ga wace tantanin halitta
Idan tantanin halitta mai tuntuɓar baya ne kawai tare da tarin zafin jiki mai ƙasa, haɗin shine dispense, sanya da warkewa, kuma ajin shine wanda aka gina don haɗin baya na BC: OSLB-1300, wanda aka ƙididdige a tantanin halitta 1,000 a kowace awa ko fiye, sanya 0.10 mm, saitin manne huɗu, gano kusurwa na CCD.
Idan mai yin tantanin hasken rana ya cancanci ɗan gajeren IR taga a kan pad ɗin, rukunin flat-ribbon ya shafi: SS-1500B, wanda ke ɗaukar ribbon 0.35 zuwa 1.0 mm faɗi da 0.12 zuwa 0.25 mm kauri a 0.15 mm sanyawa. Bambanci tsakanin su biyun ba yawan aiki ba ne. Shi ne ko tantanin hasken rana yana jure kololuwar gida.
Rukunin MBB na gefen gaba, kamar AM050FH, ba ya shafi a nan: ACM kamar yadda aka ƙaddamar da shi tsarin baya ne kawai. Idan daga baya ya koma tantanin hasken rana mai lambobin sadarwa na gefen gaba, wannan rukunin zai sake zama mai mahimmanci, ba kafin haka ba.
| Yanayin tantanin hasken rana | Abin da haɗin yake | Rukunin inji | Abin da ƙayyadaddun bayanai ke tabbatarwa |
|---|---|---|---|
| Ƙasan baya kawai mai lambobin sadarwa, tari mai ƙananan zafin jiki | Dispense manne, sanya ribbon, warkarwa | OSLB-1300 | Tsarin manne kowane pad, kololuwar warkarwa da tsayawa, 0.10 mm sanyawa |
| Ƙasan baya mai cancantar IR taga | Flat ribbon da aka narke a sandar jigilar kaya | SS-1500B | Ribbon 0.35 zuwa 1.0 mm faɗi, 0.12 zuwa 0.25 mm kauri, kololuwa a pad ɗin, 0.15 mm sanyawa |
| MBB na gefen gaba TOPCon ko PERC, ba wannan yanayin ba | Wayar zagaye da aka yi wa tausa a gaban busbars | AM050FH | Wayar 0.20 zuwa 0.26 mm, 3BB zuwa 24BB, sanya 0.05 mm |
Yadda za a rubuta shi cikin odar siya
Abubuwa biyar suna cikin ƙayyadaddun bayanai maimakon a cikin tattaunawa, domin babu ɗayansu da ke bayyana a takardar bayanan module kuma dukansu suna motsa lokacin takt.
- Zanen pad, tare da faɗin sandar jigilar kaya da tazarar lamba, domin girke-girken hangen nesa da tsarin bututun ruwa su fito daga lissafin lissafi maimakon hoto.
- Ƙarfin ja a kowane pad bayan zafi mai ɗanɗano, ba kafin ba.
- Matsakaicin zafin da ƙarfen ke jurewa da lokacin da aka ba shi.
- Ko harsashin polymer ɗin zai tsira daga sinadaran flux ɗinka, ko kuma tsarin dole ne ya kasance ba tare da flux ba.
- Sharuɗɗan EL ko PL masu shigowa, domin haɗarin karyewar yatsa dukiya ce ta tantanin halitta.
Wannan jerin shi ne wanda layin BC ya riga ya ajiye don lissafin lissafin pad ɗinsa, da ƙari ɗaya: ƙarfen yanzu yana da tarihin zafi maimakon fim ɗin da ba ya narkewa. Manne mai hana wuta a bayan shi ne irin wannan mu'amala ta farko; haɗin gwiwa shi ne na biyu.
Me zai canza tunaninmu
- Shekaru uku na bayanan filin daga wuri mai zafi da danshi, tare da buɗe modules da kuma yin bayanin emitter don jan ƙarfe.
- Bayyanar azurfa da ta rage, don haka za a iya duba alamar da lamba.
- Zafin damshi da hawan zafi na matakin module akan igiyoyin da aka haɗa da ACM, ba akan sel kawai ba.
- Ƙarfin ja bayan sa'o'i 1,000 na zafin damshi, akan ribbon da abokin ciniki zai yi amfani da shi da gaske.
Idan waɗannan sun tabbata, haɗin zai daina zama haɗari.
Inda waɗannan lambobin suka fito
Tsarin, ayyukan Layer, maganganun da aka ambata, ƙimar takaddun shaida da sharuɗɗan garanti sun fito daga bayanin fasaha na Sinanci akan dandalin ACM da aka buga a watan Oktoba 2026, wanda ya dogara da kayan ƙaddamarwa da maganganun jama'a na Li Zhenguo. Adadin ajiya da samarwa, tarihin faɗin yatsa da yanayin shekaru goma na wannan tushen ne. Rarraba, jujjuyawar kowace watt, karatun ma'aunin tsayi da taswirar inji namu ne.
Nickel silicide da titanium tungsten sun bayyana a cikin tushen a matsayin hasashe game da kayan da ba a bayyana ba, kuma sun bayyana haka a nan. Ba mu gwada, ba mu warware ko sayar da kowane sel da aka tattauna ba, kuma babu wani adadi a cikin teburin da muka auna.
Tambayoyi da Amsoshi
Tambaya: Shin da gaske ACM ba ta da azurfa?
LONGi ya bayyana shi a matsayin cikakken maye gurbin man shafawa na azurfa, amma ba a bayyana abun da ke cikinsa ba, kuma man shafawa na jan ƙarfe na iya ɗaukar ɗan azurfa a cikin iri ko Layer na lamba. Tambayi gwajin, ba siffa ba.
Tambaya: Shin tantanin ACM yana buƙatar injin ɗinka daban?
Ba wani dandali daban ba, wani kasafin kuɗi daban. Kushin da aka buga shi ne sandar gami, tarin shi ne ke ƙayyade iyaka, kuma haɗin manne ne da warkewa ko ɗan gajeren bugun wuta. Abin da ke canzawa shi ne taga, ba aji ba.
Tambaya: Za a iya ɗinka tantanin ACM da fitilar IR?
Sai idan mai yin tantanin ya tabbatar da taga a kushin. ACM yana cire matakin sintering, don haka ƙarfe ɗin ba shi da wani gefe da zai sha wuce gona da iri. Mai kaya da ya tabbatar da ɗaya zai bayyana kololuwa da lokacin jira.
Tambaya: Wane zafin jiki ne haɗin ya kamata ya kasance ƙasa da shi?
Babu lamba ɗaya, kuma duk wanda ya faɗi ɗaya yana hasashe. Iyakar tana fitowa daga tarin tantanin, kuma a kan tantanin da ke da Layer na silicon amorphous, ita ce Layer ɗin ke ƙayyade shi, ƙasa da tsarin harbi.
Tambaya: Shin mafi siraran yatsa yana canza faɗin ribbon?
Ba kai tsaye ba. Ribbon ɗin yana haɗuwa da ɓangaren jigilar, don haka faɗin yana bin tsarin pad maimakon yatsan. Abin da ke canzawa shine ƙayyadaddun ja da haƙurin sanyawa.
Tambaya: Me ya sa lantarki ɗaya ke da sassa biyu?
Saboda haɗuwar sake haɗawa tana daidaita da yankin tuntuɓar kuma juriya tana daidaita da yanki mai tsayi. Faɗin sanda a kan ƙaramin aya yana samun ƙarancin juriya da ƙaramin yankin tuntuɓa, wanda shine dukan dalilin lissafin siffar.
Tambaya: Shin ACM na sel masu tuntuɓa ta baya ne kawai?
Kamar yadda aka ƙaddamar, eh, an nufe shi ga HPBC, HIBC da BC 2.0. Sel na gefen gaba yana da wata matsala ta inuwa da mannewa daban, kuma babu wani abu a cikin kayan ƙaddamar da ke magance ta.
Tambaya: Yaushe za a sami bayanan filin?
An fara samarwa a tsakiyar 2026, don haka shekaru ɗaya zuwa uku na bayanan masana'anta yana nufin 2027 zuwa 2029, kuma kiyasin masana'antu na bayanan shekaru biyar yana kusan 2031. Har sai lokacin shaidar ita ce tsufa da aka hanzarta.
Tunani na ƙarshe
ACM yana da mahimmanci ga layin module saboda wani ɗan ƙaramin dalili. Yana ɗaukar matakin ƙarshe na zafin jiki mai girma daga metallization kuma yana sanya duk kasafin thermal a cikin haɗin, daidai lokacin da ƙarfe ya zama alloy da aka buga a ƙarƙashin harsashi na polymer. Ko jan ƙarfe zai tsaya na shekaru 25 ba shi da amsa a fili. Sayi injin da zai iya riƙe ƙaramin taga na shekaru goma.
Ga modules na back-contact tare da raguwar iyakokin thermal, OOITech tana samar da ɗaki ɗaya da biyu injin laminator na panel na hasken rana a cikin tsarin dumama mai da mai da wutar lantarki. Kayan aikinmu yana ba da daidaitaccen sarrafa zafin jiki a fadin platen don kare rear metallization mai mahimmanci. Aika zanenku, tarin module, ko samfuran gwaji zuwa ƙungiyarmu don kimanta tsari.