IEC 61215 da IEC 61730: Abin da Kowannensu Ke Tabbatarwa
Teburin Abubuwan Ciki
Amsa mai sauri: Ka'idojin biyu suna yin tambayoyi daban-daban game da samfurin guda. IEC 61215 ita ce cancantar aiki da aminci: tana rufe dorewar muhalli, ƙarfin inji da riƙe aikin lantarki, kuma ita ce ke goyan bayan da'awa game da fitarwa na dogon lokaci. IEC 61730 ita ce cancantar tsaro: tana tsara buƙatun gini sannan tana gwada rufin lantarki, haɗarin inji da halin wuta. Samfurin da zai shiga kasuwa yawanci yana buƙatar duka takaddun shaida biyu, domin babu ɗayan da ke nuna ɗayan — samfuri na iya jure tsufa cikin sauri kuma har yanzu ya kasa buƙatar tsaro, kuma samfurin mai aminci na iya lalacewa da sauri fiye da yadda takardar bayanansa ta yi alkawari.
Idan ka tuna layi ɗaya kawai daga wannan shafin: ɗaya daga cikin ka'idojin game da kasancewa da rai ne, ɗayan kuma game da kasancewa cikin aminci.

Tambayoyi Biyu, Ma'auni Biyu
IEC 61215 na tambaya ko na'urar za ta ci gaba da aiki: tana tabbatar da dorewa a hidimar waje, juriya ga lalacewa da amincin tsari a tsawon rayuwar hidima da ake auna da shekaru da yawa. IEC 61730 na tambaya ko na'urar ba ta da haɗari a zauna da ita: tana magance girgizar wutar lantarki, wuta da rauni na inji, ta hanyar buƙatu kan ginin da kuma gwaje-gwaje kan na'urar da aka gama.
Saboda tambayoyin sun bambanta, takardun sun bambanta a abin da suke kayyadewa. Ma'aunin amincin yana kayyade halayen kan lokaci; ma'aunin aminci yana kayyade abin da aka yi na'urar da kuma yadda take a yanayin kuskure da cin zarafi. Karanta takardar shaida ba tare da sanin wanne daga cikin biyun ba ba ya gaya maka kusan komai game da rabin ɗayan.
Abin da IEC 61215 Ke Gwadawa
Ma'aunin amincin yana rarraba aikinsa zuwa iyalai uku, kuma rarrabuwar tana da amfani domin tana dacewa da hanyoyi uku da na'urar ke ba wa mai ita kunya:
| Iyali | Abun ciki na yau da kullum | Abin da gazawa ke nufi |
|---|---|---|
| Dorewar muhalli | Zagayowar zafi, zafi mai danshi, daskarewar danshi, tsufan UV, hazo na gishiri da ammoniya inda ake buƙata, lalacewar da ake iya jawowa | Tsarin rufewa ko haɗin gwiwa ba ya jure yanayin da aka sayar da shi a ciki |
| Ƙarfin inji | Nauyin inji na tsaye da motsi, tasirin ƙanƙara, jurewar wuri mai zafi | Module ɗin ko hanyar haɗa shi ba ta isa ga yanayin inji ba |
| Riƙe aiki | Auna wutar farko, wuta kafin da bayan tsufa, halayen I-V, gwajin rufewa, gwajin diode na kewaye | Fitowa yana ɓacewa da sauri fiye da iyakar lalacewar da aka yarda |
Abubuwa biyu na tsarin sun cancanci sanin su domin su ne ke haifar da mafi yawan ruɗani. Na farko, an wallafa ma'aunin a sassa: buƙatun na'urar silikon crystalline suna cikin IEC 61215-2, kuma ana kiran gwaje-gwaje ɗaya-ɗaya da lambobin MQT — fallasa zafi mai ɗanɗano, alal misali, wani sashe ne da aka ayyana maimakon bayani a cikin rubutu. Na biyu, cancanta gwajin ƙira ne akan ƙira, ba garanti ba: yana nuna cewa wakilin na'urar na wannan ginin ya wuce jerin da aka ayyana, kuma canjin gini na iya sake jefa sakamakon cikin shakka.

Abin da IEC 61730 Ke Bincika
An kuma wallafa ma'aunin aminci a sassa, kuma rabon yana bayyana abin da kuke karantawa a cikin rahoto:
- Sashe na 1 — buƙatun gini. Dole ne kayan da sassan su kasance masu isa kafin a gudanar da kowane gwaji: ajin rufi na takardar baya da sauran kayan, ƙarfin firam, ƙarfin gilashi da yadda yake karyewa, ƙimar zafin akwatin haɗi, jagora da masu haɗawa, da ajin wuta da ake sa ran ginin zai cimma.
- Sashe na 2 — gwaje-gwajen aminci. Amincin lantarki ya ƙunshi juriyar rufi da juriyar wutar lantarki, da kuma juriyar zafi na akwatin haɗin wutar da amincin haɗin gwal. Amincin inji ya ƙunshi tasiri kamar gwajin faɗuwa, ƙarfin ramukan hawa, da jan igiya mai tsanani. Amincin wuta ya ƙunshi iya ƙonewa da yaɗuwar harshen wuta, kuma yana kaiwa ga darajar ajin wuta.
Dabarun rarrabewa guda biyu suna fitowa daga wannan ma'auni kuma ana rikita su akai-akai. ajin aikace-aikace yana nuna inda za a iya girka na'urar kuma wanda zai iya isa gare ta; ajin wuta yana nuna yadda ginin yake aiki a cikin wuta. Dukansu halaye ne na na'urar kamar yadda aka gina ta kuma aka girka ta — wanda shine dalilin da ya sa ake ambaton su a cikin rahoton aminci maimakon a fito da su daga takardar bayanan wutar lantarki.
Me Ya Sa Ɗaya Ba Ya Nufin Ɗayan
Takardun shaida guda biyu suna haɗa juna, kuma haɗin juna na aiki ne ba na ofis ba:
- Na'urar na iya wuce duk shirin amincin kuma har yanzu tana iya haifar da haɗarin girgiza ko wuta idan rufinta, wuraren da take da isasshen sarari ko ma'aunin zafinta bai isa ba don aikace-aikacen.
- Modulu na iya cika duk buƙatun aminci kuma har yanzu ya rasa wuta da sauri fiye da yadda aka yi alkawari, saboda babu wani abu a cikin ma'aunin aminci da ke auna lalacewa na tsawon lokaci.
- Canje-canjen gini suna motsa ma'aunin biyu daban. Sauya bayan-sheet ko akwatin haɗin wuta canji ne mai alaƙa da aminci; canza mai samar da tantanin halitta na iya zama canji mai alaƙa da aminci. Ɗaukar takardar shaidar a matsayin tana rufe “modulu” maimakon takamaiman gini da lissafin kayan aiki shine kuskure mafi yawa a cikin fayil ɗin saye.
Iyaka: Waɗanne Modulu, Wanne Buga
Duk ma'aunin biyu sun shafi modulun silikon crystalline da na fim na bakin ciki, tare da buƙatun modulun silikon crystalline a cikin sashe na –2 na IEC 61215. Fasahar tantanin halitta da ke kasuwa a yanzu — TOPCon, HJT, nau'ikan back-contact da sauran su — suna cikin tsarin cancanta ɗaya; abin da ke canzawa shine yadda wani gini ke aiki a ƙarƙashin gwaje-gwajen, ba wace ma'auni ke shafi shi ba.
Bugu suna da mahimmanci kamar lambar ma'auni. An sake duba yanayin gwaji da ka'idojin cin nasara tsawon shekaru, don haka ya kamata a karanta takardar shaidar tare da shekararta, kuma a kwatanta ta da shekarar da ƙayyadaddun mai siye ya ambata. Buƙatar zafi mai ɗanɗano misali ne mai kyau na yanayin da ya tsaya tsayin daka tsawon shekaru ashirin yayin da tsammanin kasuwa game da shi bai tsaya ba.
Yadda Ake Samar da Shaida
Takardar shaidar ita ce ƙarshen sarkar: ma'auni yana bayyana gwaji da iyaka, wani kayan aiki yana samar da ma'auni, rahoto yana rubuta shi bisa wani sashe, kuma ƙungiyar ba da takardar shaidar tana mai da shi takardar shaidar wani gini da aka ayyana. Fahimtar wace hanyar da masana'anta ke sarrafawa ita ce ke sa shirin ba da takardar shaidar ya zama mai gaskiya.
Wasu daga cikin sarkar ana ajiye su a cikin gida akai-akai: dubawa da ido, electroluminescence da auna I-V, gwajin rufewa da jurewa, duba bypass diode da gwaje-gwajen yau da kullum da ke biyo kowane module daga layin. A nan ne masu gwaji kamar PV safety comprehensive tester ko hipot insulation resistance tester zauna, saboda suna goyan bayan shaidar amincin lantarki da ma'aunin aminci ke nema. Tsawon lokaci na tsufa, ƙanƙara, nauyin inji, PID da gwajin wuta yawanci ana kai su zuwa dakin gwaje-gwaje mai cancanta tare da ɗakunan da aka tabbatar da ma'aunin da aka daidaita.

Jerin kayan aiki da ke bayan ɓangaren aminci — ɗakunan yanayi, ɗakunan UV, tsarin PID, na'urorin nauyin inji, na'urorin gwajin ƙanƙara da na'urorin kwaikwayo — an bayyana su a cikin Bayani kan kayan gwajin takardar shaida na IEC, kuma ana bayanin kowane gwaji a ɓangaren aminci a cikin Gwaje-gwajen amincin module na PV.
Yadda ake Karanta Takardar Shaida ko Rahoto
Abubuwa shida suna mai da takardar shaida daga shafi a cikin fayil ɗin tayin zuwa bayani mai amfani: ma'aunin lamba da shekarar bugu; waɗanne sassa aka rufe (61215-2, 61730-1 da 61730-2); da gini da lissafin kayan aiki takardar shaidar da ta shafi, gami da nau'ikan module; da ajin aikace-aikace da ajin wuta inda suka dace; da dakin gwaje-gwaje da amincewa bayan rahoton gwajin; da duk wani sabani ko keɓancewa da aka rubuta. Idan mai bayarwa ba zai iya nuna ginin da aka rufe ba, takardar shaidar ba ta canjawa zuwa module da ake ambato ba.
Tambayoyi da Amsoshi
Menene bambanci tsakanin IEC 61215 da IEC 61730 a jumla ɗaya?
IEC 61215 tana tabbatar da ko module ɗin zai ci gaba da aiki a tsawon rayuwarsa; IEC 61730 tana tabbatar da ko yana da aminci dangane da girgizar lantarki, haɗarin inji da wuta.
Shin ina buƙatar duka takaddun shaida biyu don sayar da module?
A yawancin kasuwanni, eh. Su biyu cancanta ne daban-daban da ke da fannoni daban-daban, kuma masu siye yawanci suna neman duka biyun kafin su karɓi module cikin aiki.
Shin wucewa a IEC 61215 zai iya maye gurbin IEC 61730?
A'a. Shirin amincin ba ya gwada halin wuta kuma ba ya saita buƙatun gini da ma'aunin aminci ya gindaya, don haka ba zai iya maye gurbinsa ba.
Menene ajin wuta a takardar shaidar module?
Yana bayyana yadda ginin module yake aiki game da yaduwar harshen wuta da konewa, kuma ya fito daga gwajin wuta na ma'aunin aminci. Mallakin gini ne da yadda ake ɗora module ɗin, ba na fasahar tantanin halitta kaɗai ba.
Menene ajin aikace-aikace?
Rabe-rabe a cikin ma'aunin aminci da ke nuna inda za a iya shigar da module ɗin da kuma wanda zai iya saduwa da shi, wanda hakan ke shafar buƙatun rufi da samun dama da ya kamata ya cika.
Shin canza wani sashe yana lalata takardar shaidar?
Zai iya. Ana bayar da takaddun shaida don gini da lissafin kayan da aka ayyana, don haka canji ga wani sashe mai alaƙa da aminci kamar bayan-shafi ko akwatin haɗin wuta dole a tantance shi da takardar shaidar maimakon a ɗauka an rufe shi.
Tunani na Ƙarshe
Ka ɗauki ma'aunai biyu a matsayin akwatunan ajiya biyu, ba nau'ikan takarda ɗaya ba. IEC 61215 tana riƙe da shaidar cewa module ɗin yana dawwama; IEC 61730 tana riƙe da shaidar cewa yana da aminci, gami da buƙatun gini da ke bayansa. Lokacin da kake duba fayil ɗin mai bayarwa, duba wace ma'auni kowane takarda yake ciki, wace bugu aka fitar da ita, da wane gini take rufewa — waɗannan tambayoyi uku suna warware yawancin ruɗani da ke tattare da waɗannan lambobi biyu.
Masu alaƙa: yadda ka'idojin PV suka shafi juna taswirori IEC, EN, UL da kuma matakan ka'idojin Sin, kuma yana bayanin inda tilastawa bayan kowannensu ya fito.
Masu alaƙa: IEC TS 62915 da sake gwada na'ura yana bayyana waɗanne canje-canje ne ke tilasta waɗanne gwaje-gwaje, da kuma yadda ake ci gaba da takardar shaidar da take akwai.
Masu alaƙa: TOPCon UVID da r-UVID / ir-UVID rabuwa yana nuna abin da matakin riga-kafin UV a cikin IEC 61215 ya ƙunsa kuma bai ƙunsa ba a matakin tantanin halitta.
Masu alaƙa: Perovskite a sararin samaniya: abin da zagayowar girgizar zafi 100 ke kashewa ita ce ma'aunin da iyakar zagayowar zafi ta kewayawa ya zarce kusan sau huɗu.
Ƙarin karatu da bayanan baya